Mortazavi Vajihesadat, Samimi Pouran, Rafizadeh Mojgan, Kazemi Shantia
Torabinejad Dental Research Center and Department of Operative Dentistry, Isfahan University of Medical Sciences, Isfahan, Iran.
Dent Res J (Isfahan). 2012 Sep;9(5):588-94. doi: 10.4103/1735-3327.104878.
Composite resin restorations may have a short lifespan due to the degradation of resin-dentin interface. Ethanol wet bonding technique may extend the longevity of resin-dentin bond. The purpose of this one year randomized clinical trial was to compare clinical performance of two adhesives with ethanol wet bonding technique.
This randomized clinical trial was performed on 36 non-carious cervical lesions in 12 patients restored with composite resin using one of the following approaches: 1. OptiBond FL (Kerr, USA); 2. Clearfil SE Bond (Kuraray, Japan) with enamel etching and 3. Ethanol wet bonding technique with the part of adhesive of OptiBond FL. The clinical success rate was assessed after 24 h, 6, 9 and 12 months according to the United States Public Health Service (USPHS) criteria: Marginal discoloration, marginal defect, retention rate, caries occurrence, and postoperative sensitivity. The tooth vitality was also assessed.
The retention rate was 100% at baseline and at 6 months follow up for all types of bonding protocols and was 91.67% at 9 and 12 months follow up for ethanol wet bonding group. None of the restorations in three groups showed marginal defects, marginal discoloration or caries occurrence and were vital after 12 months. There was no statistically significant difference between three groups after 12 months follow up (p value = 0.358).
Composite restorations placed using ethanol wet bonding technique presented equal performance to the other groups.
由于树脂-牙本质界面的降解,复合树脂修复体的使用寿命可能较短。乙醇湿粘结技术可能会延长树脂-牙本质粘结的寿命。这项为期一年的随机临床试验的目的是比较两种采用乙醇湿粘结技术的粘结剂的临床性能。
对12例患者的36个非龋性颈部病变进行了这项随机临床试验,采用以下方法之一用复合树脂进行修复:1. OptiBond FL(美国 Kerr 公司);2. 采用釉质酸蚀的 Clearfil SE Bond(日本可乐丽公司);3. 用 OptiBond FL 的部分粘结剂进行乙醇湿粘结技术。根据美国公共卫生服务(USPHS)标准,在24小时、6个月、9个月和12个月后评估临床成功率:边缘变色、边缘缺损、保留率、龋病发生情况和术后敏感性。还评估了牙齿活力。
所有粘结方案在基线和6个月随访时的保留率均为100%,乙醇湿粘结组在9个月和12个月随访时的保留率为91.67%。三组修复体均未出现边缘缺损、边缘变色或龋病发生,12个月后均有活力。12个月随访后三组之间无统计学显著差异(p值 = 0.358)。
采用乙醇湿粘结技术放置的复合修复体与其他组表现相当。