基于流动注射微柱预富集与石墨炉原子吸收光谱联用,制备和表征磁性纳米粒子用于在线测定矿样中的金、钯和铂。

Preparation and characterization of magnetic nanoparticles for the on-line determination of gold, palladium, and platinum in mine samples based on flow injection micro-column preconcentration coupled with graphite furnace atomic absorption spectrometry.

机构信息

College of Chemistry, Jilin University, Changchun 130012, PR China.

出版信息

Talanta. 2014 Jan;118:231-7. doi: 10.1016/j.talanta.2013.10.018. Epub 2013 Oct 18.

Abstract

A simple and highly selective procedure for on-line determination of trace levels of Au, Pd, and Pt in mine samples has been developed using flow injection-column adsorption preconcentration coupled with graphite furnace atomic absorption spectrophotometry (FI-column-GFAAS). The precious metals were adsorbed on the as-synthesized magnetic nanoparticles functionalized with 4'-aminobenzo-15-crown-5-ether packed into a micro-column and then eluted with 2% thiourea + 0.1 mol L(-1) HCl solution prior to the determination by GFAAS. The properties of the magnetic adsorbents were investigated by scanning electron microscope (SEM), X-ray diffraction (XRD), and vibrating sample magnetometer (VSM). Various experimental parameters affecting the preconcentration of Au, Pd, and Pt were investigated and optimized. Under the optimal experimental conditions, the detection limits of the developed technique were 0.16 ng mL(-1) for Au, 0.28 ng mL(-1) for Pd, and 1.01 ng mL(-1) for Pt, with enrichment factors of 24.3, 13.9, and 17.8, respectively. Precisions, evaluated as repeatability of results, were 1.1%, 3.9%, and 4.4% respectively for Au, Pd, and Pt. The developed method was validated by the analysis of Au, Pd, and Pt in certified reference materials and mine samples with satisfactory results.

摘要

一种简单且高选择性的程序,用于在线测定矿样中痕量金、钯和铂,已采用流动注射柱吸附预浓缩结合石墨炉原子吸收分光光度法(FI-柱-GFAAS)开发。将贵金属吸附在合成的磁性纳米颗粒上,这些纳米颗粒用 4'-氨基苯并-15-冠-5-醚功能化,填充到微柱中,然后用 2%硫脲+0.1mol/L HCl 溶液洗脱,再用 GFAAS 进行测定。通过扫描电子显微镜(SEM)、X 射线衍射(XRD)和振动样品磁强计(VSM)研究了磁性吸附剂的性质。研究并优化了影响 Au、Pd 和 Pt 预浓缩的各种实验参数。在最佳实验条件下,该技术的检测限分别为 Au 为 0.16ng/mL、Pd 为 0.28ng/mL、Pt 为 1.01ng/mL,富集因子分别为 24.3、13.9 和 17.8。Au、Pd 和 Pt 的重复性分别为 1.1%、3.9%和 4.4%。该方法通过对金、钯和铂标准参考物质和矿样的分析进行了验证,结果令人满意。