A series of polyvinyl alcohol (PVA), PVA/chitosan (CS) and PVA/cyanobacterial extracellular polymeric substances (EPS) blended nanofibrous membranes were produced by electrospinning using a microfiltration poly(vinylidene fluoride) (PVDF) basal membrane, for potential applications in water filtration. Nanofibres were obtained from solutions of 20% (w/w) PVA with 1% (w/w) CS or EPS, using a weight ratio of 60/40. Blended nanofibres have shown a smooth morphology, no beads formation and diameters between 50 and 130 nm. Thermo-mechanical analysis demonstrated that there were inter and/or intramolecular hydrogen bonds between the molecules of PVA/CS and PVA/EPS in the blends. The electrospun blended PVA/EPS membrane showed better tensile mechanical properties when compared with PVA and PVA/CS, and resisted more against disintegration in the temperature range between 10 and 50 °C. Finally, the blended membranes have shown an increase in chromium binding capacity of 5%. This is the first successful report of a blended membrane of electrospinned cyanobacterial polysaccharide with PVA.

摘要

一系列聚乙烯醇(PVA)、PVA/壳聚糖(CS)和 PVA/蓝藻细胞外聚合物(EPS)共混纳米纤维膜通过静电纺丝由微滤聚偏二氟乙烯(PVDF)基膜制备而成,用于潜在的水过滤应用。纳米纤维由 20%(w/w)PVA 与 1%(w/w)CS 或 EPS 的溶液制成,使用 60/40 的重量比。共混纳米纤维具有光滑的形态,没有珠形成,直径在 50 和 130nm 之间。热机械分析表明,在共混物中 PVA/CS 和 PVA/EPS 的分子之间存在分子间和/或分子内氢键。与 PVA 和 PVA/CS 相比,静电纺丝共混 PVA/EPS 膜具有更好的拉伸力学性能,并且在 10 至 50°C 的温度范围内更能抵抗分解。最后,共混膜的铬结合能力增加了 5%。这是首次成功报道 PVA 与蓝藻多糖共混静电纺丝膜。