Tanomaru-Filho Mario, Bosso Roberta, Viapiana Raqueli, Guerreiro-Tanomaru Juliane M
Department of Restorative Dentistry, Araraquara School of Dentistry, UNESP - Univ Estadual Paulista, Araraquara, SP, Brazil.
Acta Odontol Latinoam. 2013;26(2):121-5.
The present study evaluated the radiopacity and flow of different endodontic sealers: AH Plus, Endo CPM, MTA Fillapex, Sealapex, Epiphany, and Epiphany SE. For the radiopacity test, six specimens measuring 10 mm in diameter and 1 mm in thickness were fabricated from each material. They were radiographed on an occlusal film alongside an aluminum step wedge. Radiographs were digitized to determine the radiopacity equivalence in millimeters of aluminum. To evaluate the flow, a 120 g load was placed on top of a glass slab containing 0.05 +/- 0.005 mll of sealer. The diameters of each material were measured (mm) with a caliper and samples were photographed. Digitized images were analyzed using the UTHSCSA Image Tool for Windows software, to determine the sealer area (mm2). Data were submitted to ANOVA and Tukey's test at 5% significance. AH Plus and Epiphany SE presented the greatest radiopacity (12.5 mm Al and 12.0 mm Al, respectively) (p > 0.05), followed by Epiphany (9.6 mm Al) and Fillapex (8.9 mm Al). Endo CPM (5.46 mm Al) and Sealapex (5.51 mm Al) presented lower radiopacity. MTA Fillapex presented significantly higher values of flow than other sealers (33.11 mm and 844.9 mm2). AH Plus, Epiphany, and Epiphany SE had similar values. Endo CPM (21.05 mm and 342.8 mm2) and Sealapex (19.98 mm and 352.5 mm2) presented the lowest flow values (p > 0.05). All sealers presented radiopacity and flow values according to ISO and ANSI/ADA recommendations.
AH Plus、Endo CPM、MTA Fillapex、Sealapex、Epiphany和Epiphany SE。对于射线不透性测试,每种材料制作六个直径10毫米、厚度1毫米的样本。将它们与铝阶梯楔形块一起放在咬合片上进行射线照相。射线照片数字化以确定铝毫米数的射线不透性等效值。为评估流动性,在含有0.05±0.005毫升封闭剂的玻璃板上放置120克负荷。用卡尺测量每种材料的直径(毫米)并对样本拍照。使用适用于Windows的UTHCSA Image Tool软件分析数字化图像,以确定封闭剂面积(平方毫米)。数据进行方差分析和5%显著性的Tukey检验。AH Plus和Epiphany SE呈现出最大的射线不透性(分别为12.5毫米铝和12.0毫米铝)(p>0.05),其次是Epiphany(9.6毫米铝)和Fillapex(8.9毫米铝)。Endo CPM(5.46毫米铝)和Sealapex(5.51毫米铝)呈现出较低的射线不透性。MTA Fillapex呈现出比其他封闭剂显著更高的流动性值(33.11毫米和844.9平方毫米)。AH Plus、Epiphany和Epiphany SE具有相似的值。Endo CPM(21.05毫米和342.8平方毫米)和Sealapex(19.98毫米和352.5平方毫米)呈现出最低的流动性值(p>0.05)。所有封闭剂的射线不透性和流动性值均符合ISO和ANSI/ADA的建议。