ACS Appl Mater Interfaces. 2014 Feb 12;6(3):1740-6. doi: 10.1021/am404709w. Epub 2014 Jan 29.
Pore-enlarged mesoporous silica nanoparticles (MSNs) were prepared directly from as-prepared MSNs through a new, simple method using divalent Ca or Mg salts as both efficient silica etching reagents and as ion exchangers in methanolic solution under mild conditions. The resultant MSNs became almost template-free simultaneously during this etching process. The pore-enlarged MSNs, referred to as Ca-MSN or Mg-MSN, maintained their original hexagonal pore symmetry and particle sizes, but several ultra-large mesopores were generated inside and outside the MSNs together with regular mesopores having expanded pore dimension of around 4-5 nm. The average pore diameters for ultra-large pores were 47.5 nm for Ca-MSN and 52.4 nm for Mg-MSN. The generation of ultra-large pores can be regarded as the collapse of several mesopores into an ultra-large pore. Both Ca-MSN and Mg-MSN were good sorbents for positively charged porphyrin molecules. Additionally, these ultra-large pore MSNs exhibited better adsorption ability than calcined MSN for large proteins and antibodies, such as bovine serum albumin (BSA) and immunoglobulin G (IgG).
大孔介孔硅纳米粒子(MSNs)可通过一种新的简单方法直接从所制备的 MSNs 中制备得到,该方法使用二价 Ca 或 Mg 盐作为高效的硅蚀刻试剂,并在甲醇溶液中作为离子交换剂,在温和条件下进行。在这个蚀刻过程中,所得的 MSNs 几乎同时变成无模板。这种大孔 MSNs 被称为 Ca-MSN 或 Mg-MSN,它们保持了原始的六方孔对称性和颗粒尺寸,但在 MSNs 内外同时产生了几个超大介孔,同时具有扩展的约 4-5nm 的孔尺寸的规则介孔。超大孔的平均孔径为 47.5nm 的 Ca-MSN 和 52.4nm 的 Mg-MSN。超大孔的产生可以看作是几个介孔塌陷成一个超大孔。Ca-MSN 和 Mg-MSN 都是正电荷卟啉分子的良好吸附剂。此外,这些超大孔 MSNs 对大蛋白和抗体(如牛血清白蛋白(BSA)和免疫球蛋白 G(IgG))的吸附能力优于煅烧 MSN。