Shirinzad M, Ebadi Sh, Shokripour M, Darabi Ma
Dept. of Operative Dentistry, School of Dentistry, Hamedan University of Medical Science, Hamedan, Iran.
Dept. of Operative Dentistry, School of Dentistry, Ghazvin University of Medical Science, Ghazvin, Iran.
J Dent (Shiraz). 2014 Mar;15(1):22-7.
A strong bond of fiber post to resin core, as well as to dentin would critically ensure the durability of restorations in endodontically treated teeth.
The purpose of this study was to evaluate the effect of etch-and-rinse dentin bonding systems on the bond strength between resin core and fiber post after application of 24% hydrogen peroxide.
24 fiber posts (RTD; St. Egèven, France) were treated with 24% hydrogen peroxide for 10 minutes. They were randomly divided into 4 groups (n=6) based on the bonding agent used: Group P: Prime&Bond, Group O: One Step, Group S: Single Bond and Group E: Excite. Each group was prepared according to the manufacturer's instructions. For all posts, a flowable composite core (ÆliteFlo; Bisco, USA) was built-up over the bonded area. Each specimen was sectioned to produce 2 sticks, 1mm in thickness and underwent microtensile bond strength (µTBS). Data were analyzed using one-way ANOVA at the 0.05 level. The fractured surfaces of all sticks were evaluated by stereomicroscope (× 20). Scanning electron microscopy(SEM) assessment of two sticks from each group was performed to evaluate the surface morphology.
The means and SDs of µTBS were: Group P: 10.95±1.74; Group S: 10.25±2.39; Group E: 9.52±2.07; and Group O: 9.12±1.34. There was no statistically significant difference in bond strength means between the groups tested (p> 0.05).
The results of this study indicated the bonding agents used had no significant influence on the bond strength of fiber post to composite core.
纤维桩与树脂核以及牙本质之间的牢固结合对于确保根管治疗后牙齿修复体的耐久性至关重要。
本研究的目的是评估酸蚀冲洗牙本质粘结系统在应用24%过氧化氢后对树脂核与纤维桩之间粘结强度的影响。
24根纤维桩(RTD;法国圣埃热万)用24%过氧化氢处理10分钟。根据所使用的粘结剂将它们随机分为4组(n = 6):P组:Prime&Bond;O组:One Step;S组:Single Bond;E组:Excite。每组均按照制造商的说明进行制备。对于所有桩,在粘结区域上堆积流动复合树脂核(ÆliteFlo;美国Bisco)。每个标本切成2根厚度为1mm的棒,并进行微拉伸粘结强度(µTBS)测试。数据采用单因素方差分析,检验水准为0.05。所有棒的断裂面用体视显微镜(×20)评估。对每组的两根棒进行扫描电子显微镜(SEM)评估以观察表面形态。
µTBS的均值和标准差分别为:P组:10.95±1.74;S组:10.25±2.39;E组:9.52±2.07;O组:9.12±1.34。所测试组之间的粘结强度均值无统计学显著差异(p>0.05)。
本研究结果表明所使用的粘结剂对纤维桩与复合树脂核之间的粘结强度没有显著影响。