Sfondrini Maria F, Fraticelli Danilo, Castellazzi Linda, Scribante Andrea, Gandini Paola
MD, DDS, PhD. Università degli Studi di Pavia - Dipartimento di Scienze Clinico-Chirurgiche, Diagnostiche e Pediatriche, Sezione di Odontoiatria, UDA di Ortognatodonzia e Odontoiatria Infantile. Italy.
MD, PhD. Università degli Studi di Pavia - Dipartimento di Scienze Clinico-Chirurgiche, Diagnostiche e Pediatriche, Sezione di Odontoiatria, UDA di Ortognatodonzia e Odontoiatria Infantile. Italy.
J Clin Exp Dent. 2014 Apr 1;6(2):e145-9. doi: 10.4317/jced.51379. eCollection 2014 Apr.
The purpose of this longitudinal prospective randomized study was to evaluate the clinical reliability of two different types of postorthodontic treatment retainers: a silanised-treated glass fibers-reinforced resin composite (FRC) and a directly bonded multistranded stainless steel wire. The hypothesis of the study was to assess if significant differences are present between failure rates of the two retainers.
This prospective study was based on an assessment of 87 patients (35 men and 52 women),with an average age of 24 years who required a lower arch fixed retainer after orthodontic treatment. Patients were divided in two groups. Assignment was carried out with random tables. A follow-up examination was carried out once a month. The number, cause, and date of single bond adhesive failures were recorded for both retainers over 12 months. Teeth that were rebonded after failure were not included in the success analysis. Statistical analysis was performed by means of a Fisher's exact test, Kaplan-Meier survival estimates, and log rank test.
Bond failure rate was significantly higher (P=0.0392) for multistranded metallic wire than for FRC.
Glass fiber-reinforced resin composite retainers and multistranded metallic wires showed no significant difference in single bond failure rates over a one-year follow up. Key words:Fiber reinforced composite, fixed retention, multistranded wire, orthodontics, retainer, splint.
本纵向前瞻性随机研究旨在评估两种不同类型的正畸治疗后保持器的临床可靠性:硅烷化处理的玻璃纤维增强树脂复合材料(FRC)和直接粘结的多股不锈钢丝。本研究的假设是评估两种保持器的失败率之间是否存在显著差异。
本前瞻性研究基于对87例患者(35名男性和52名女性)的评估,这些患者平均年龄为24岁,正畸治疗后需要在下颌弓使用固定保持器。患者被分为两组。通过随机表进行分组。每月进行一次随访检查。记录两种保持器在12个月内的单粘结剂失败数量、原因和日期。失败后重新粘结的牙齿不纳入成功分析。采用Fisher精确检验、Kaplan-Meier生存估计和对数秩检验进行统计分析。
多股金属丝的粘结失败率显著高于FRC(P=0.0392)。
在一年的随访中,玻璃纤维增强树脂复合材料保持器和多股金属丝在单粘结失败率方面没有显著差异。关键词:纤维增强复合材料、固定保持、多股丝、正畸、保持器、夹板。