Suppr超能文献

用于正畸粘接的瓷贴面预处理:扫描电子显微镜-能谱分析

Porcelain laminate veneer conditioning for orthodontic bonding: SEM-EDX analysis.

作者信息

Aksakalli Sertac, Ileri Zehra, Yavuz Tevfik, Malkoc Meral Arslan, Ozturk Nilgun

机构信息

Department of Orthodontics, Bezmialem Vakif University, Istanbul, Turkey,

出版信息

Lasers Med Sci. 2015 Sep;30(7):1829-34. doi: 10.1007/s10103-014-1682-5. Epub 2014 Oct 26.

Abstract

The purpose of this in vitro study was to evaluate and compare the effects of different surface treatments and laser irradiation on the bond strength of brackets bonded to porcelain laminate veneer. Porcelain laminate veneer specimens were embedded in the centers of acrylic resin blocks. Thirty-nine teeth were used for shear bond strength testing and the remaining three (one tooth for each group) were used for evaluation of the debonded bracket interface. Specimens were randomly divided into three groups, each containing 13 specimens. The details of the groups are as follows: Group SB, sandblasting with alumina particles (50 μm); Group HFA, 9.6 % hydrofluoric acid etching; Group ER, erbium-doped yttrium-aluminum-garnet (Er: YAG) irradiation (from 1 mm distance, 2 W, 10 Hz for 10 s). After conditioning, the upper central brackets were bonded to the porcelain surfaces. Porcelain laminate veneers were examined under stereomicroscope for adhesive remnant index and surface damage after debonding. The highest shear bond strength values were obtained with Group HFA (10.8 ± 3.8 MPa) and Group ER (9.3 ± 1.5 MPa), whereas Group SB revealed the lowest values. Scanning electron microscopy energy-dispersive X-ray (SEM-EDX) analysis revealed that the silicon level in the porcelain decreased after debonding in all groups. The sandblasting method did not demonstrate any ideal bond strength values; however, the 9.6 % hydrofluoric acid etching and Er: YAG laser did. There were no significant differences among all groups in terms of laminate surface damages. The Er: YAG laser therefore can be selected for ideal bond strength and minimal damage to porcelain laminates.

摘要

本体外研究的目的是评估和比较不同表面处理及激光照射对粘结于烤瓷贴面的托槽粘结强度的影响。将烤瓷贴面标本嵌入丙烯酸树脂块中心。39颗牙齿用于剪切粘结强度测试,其余三颗(每组一颗)用于评估脱粘托槽界面。标本随机分为三组,每组13个标本。各组详细情况如下:SB组,用氧化铝颗粒(50μm)喷砂;HFA组,9.6%氢氟酸蚀刻;ER组,掺铒钇铝石榴石(Er:YAG)激光照射(距离1mm,2W,10Hz,照射10s)。处理后,将上颌中切牙托槽粘结于瓷表面。脱粘后,在体视显微镜下检查烤瓷贴面的粘结残留指数和表面损伤情况。HFA组(10.8±3.8MPa)和ER组(9.3±1.5MPa)获得的剪切粘结强度值最高,而SB组的值最低。扫描电子显微镜能谱X射线(SEM-EDX)分析显示,脱粘后所有组瓷中的硅含量均降低。喷砂法未显示出任何理想的粘结强度值;然而,9.6%氢氟酸蚀刻和Er:YAG激光显示出了理想值。在所有组中,贴面表面损伤方面无显著差异。因此,Er:YAG激光可因其理想的粘结强度和对烤瓷贴面的最小损伤而被选用。