Canellas E, Vera P, Nerín C
GUIA Group, Department of Analytical Chemistry, University of Zaragoza, I3A, María de Luna,3, 50018 Zaragoza, Spain; Samtack Adhesivos Industriales, C/ Cerámica, n°3, Pol. Ind. Magarola Sud, 08292, Esparreguera, Barcelona, Spain.
GUIA Group, Department of Analytical Chemistry, University of Zaragoza, I3A, María de Luna,3, 50018 Zaragoza, Spain.
Food Chem Toxicol. 2015 Jan;75:79-87. doi: 10.1016/j.fct.2014.10.029. Epub 2014 Nov 13.
Adhesives are used to manufacture multilayer materials, where their components pass through the layers and migrate to the food. Nine different adhesives (acrylic, vinyl and hotmelt) and their migration in 21 laminates for future use as market samples have been evaluated and risk assessment has been carried out. A total of 75 volatiles and non volatile compounds were identified by gas chromatography-mass spectrometry and ultra-performance liquid chromatography coupled to quadrupole time-of-flight mass spectrometry. Most of the compounds migrated below their specific migration limit (SML), lowest observed adverse effect level (LOAEL), no observed adverse effect level (NOAEL) and values recommended by Cramer. Six compounds classified as high toxicity class III according to Cramer classification, migrated over their SML and exposure values recommended by Cramer, when they were applied in the full area of the packaging. Nevertheless, these adhesives fulfill the threshold in the real application as they are applied in a small area of the packaging.
粘合剂用于制造多层材料,其成分会穿过各层并迁移到食品中。已对九种不同的粘合剂(丙烯酸类、乙烯基类和热熔类)及其在21种用作市场样品的层压板中的迁移情况进行了评估,并开展了风险评估。通过气相色谱-质谱联用仪和超高效液相色谱-四极杆飞行时间质谱联用仪共鉴定出75种挥发性和非挥发性化合物。大多数化合物的迁移量低于其特定迁移限量(SML)、最低观察到有害作用水平(LOAEL)、未观察到有害作用水平(NOAEL)以及克莱默推荐的值。根据克莱默分类法,有六种化合物被归类为高毒性III类,当它们应用于包装的整个区域时,其迁移量超过了SML和克莱默推荐的暴露值。然而,这些粘合剂在实际应用中满足阈值要求,因为它们仅应用于包装的小面积区域。