Xiao Wenge, Zhang Xia, Hao Zhendong, Pan Guo-Hui, Luo Yongshi, Zhang Ligong, Zhang Jiahua
†State Key Laboratory of Luminescence and Applications, Changchun Institute of Optics, Fine Mechanics and Physics, Chinese Academy of Sciences, Changchun 130033, China.
‡University of Chinese Academy of Sciences, Beijing 100049, China.
Inorg Chem. 2015 Apr 6;54(7):3189-95. doi: 10.1021/ic502773t. Epub 2015 Mar 9.
Novel blue-emitting K2Al2B2O7:Eu(2+) (KAB:Eu(2+)) phosphor was synthesized by solid state reaction. The crystal structural and photoluminescence (PL) properties of KAB:Eu(2+) phosphor, as well as its thermal properties of the photoluminescence, were investigated. The KAB:Eu(2+) phosphor exhibits broad excitation spectra ranging from 230 to 420 nm, and an intense asymmetric blue emission band centered at 450 nm under λex = 325 nm. Two different Eu(2+) emission centers in KAB:Eu(2+) phosphor were confirmed via their fluorescence decay lifetimes. The optimal concentration of Eu(2+) ions in K2-xEuxAl2B2O7 was determined to be x = 0.04 (2 mol %), and the corresponding concentration quenching mechanism was verified to be the electric dipole-dipole interactions. The PL intensity of the nonoptimized KAB:0.04Eu(2+) phosphor was measured to be ∼58% that of the commercial blue-emitting BaMgAl10O17:Eu(2+) phosphor, and this phosphor has high color purity with the CIE coordinate (0.147, 0.051). When heated up to 150 °C, the KAB:0.04Eu(2+) phosphor still has 82% of the initial PL intensity at room temperature, indicating its high thermal stability. These results suggest that the KAB:Eu(2+) is a promising candidate as a blue-emitting n-UV convertible phosphor for application in white light emitting diodes.
通过固相反应合成了新型蓝色发光的K2Al2B2O7:Eu(2+)(KAB:Eu(2+))荧光粉。研究了KAB:Eu(2+)荧光粉的晶体结构、光致发光(PL)特性及其光致发光的热性能。KAB:Eu(2+)荧光粉在230至420nm范围内呈现出宽激发光谱,在λex = 325nm下,在450nm处有一个强烈的不对称蓝色发射带。通过荧光衰减寿命证实了KAB:Eu(2+)荧光粉中存在两个不同的Eu(2+)发射中心。确定K2-xEuxAl2B2O7中Eu(2+)离子的最佳浓度为x = 0.04(2mol%),并验证相应的浓度猝灭机制为电偶极-偶极相互作用。测量未优化的KAB:0.04Eu(2+)荧光粉的PL强度约为商用蓝色发光BaMgAl10O17:Eu(2+)荧光粉的58%,该荧光粉具有高色纯度,CIE坐标为(0.147, 0.051)。当加热到150°C时,KAB:0.04Eu(2+)荧光粉在室温下仍具有初始PL强度的82%,表明其具有高热稳定性。这些结果表明,KAB:Eu(2+)作为一种用于白光发光二极管的蓝色发射近紫外可转换荧光粉是一个有前途的候选材料。