用于pH可切换生物传感的血红蛋白与多壁碳纳米管之间的逐层组装膜。

Layer by layer assembled films between hemoglobin and multiwall carbon nanotubes for pH-switchable biosensing.

作者信息

Pan Zhongqin, Liu Xiaojun, Xie Jing, Bao Ning, He Hong, Li Xiaodong, Zeng Jiang, Gu Haiying

机构信息

Institute of Analytical Chemistry for Life Science, Nantong University, Nantong 226019, China; School of Public Health, Nantong University, Nantong 226019, China.

Institute of Analytical Chemistry for Life Science, Nantong University, Nantong 226019, China; School of Public Health, Nantong University, Nantong 226019, China; Affiliated Hospital, Nantong University, Nantong 226021, China.

出版信息

Colloids Surf B Biointerfaces. 2015 May 1;129:169-74. doi: 10.1016/j.colsurfb.2015.03.044. Epub 2015 Mar 27.

Abstract

Although pH-switchable behaviors have been reported based on multilayer films modified electrodes, their pH-switchable biosensing is still difficult due to the existence of the electroactive mediator. In this study, we report the pH-dependable determination of hydrogen peroxide (H2O2) based on a four-bilayer film fabricated through layer by layer assembly between hemoglobin (Hb) and multiwall carbon nanotubes (MWCNTs). We observed that response of electroactive probe Fe(CN)6(3-) at the multilayer films was very sensitive and reversible to pH values of phosphate buffer solutions phosphate buffer solution with cyclic voltammetry. The reduction peak height of Fe(CN)6(3-) at the multilayer film could reach ∼221μA at pH 3.0 while 0μA at pH 9.0. The linear range for the detection of H2O2 at pH 3.0 was from 12.5μM to 10.4mM, which was much wider than that at pH 9.0. Our results demonstrated that the detection of H2O2 with the proposed modified electrode is dependent on pH values of phosphate buffer solution. Moreover, the component of multilayer films has impacts on the performance of biosensors with pH-switchable behaviors.

摘要

尽管基于多层膜修饰电极已报道了pH可切换行为,但由于电活性介质的存在,其pH可切换生物传感仍很困难。在本研究中,我们报道了基于通过血红蛋白(Hb)和多壁碳纳米管(MWCNT)之间的层层组装制备的四层膜对过氧化氢(H2O2)进行pH依赖性测定。我们通过循环伏安法观察到,多层膜上电活性探针Fe(CN)6(3-)的响应对磷酸盐缓冲溶液的pH值非常敏感且可逆。在pH 3.0时,多层膜上Fe(CN)6(3-)的还原峰高可达约221μA,而在pH 9.0时为0μA。在pH 3.0时检测H2O2的线性范围为12.5μM至10.4mM,比在pH 9.0时宽得多。我们的结果表明,用所提出的修饰电极检测H2O2取决于磷酸盐缓冲溶液的pH值。此外,多层膜的组成对具有pH可切换行为的生物传感器的性能有影响。