Castellano-Hernández Elena, Han Xiumei, Rico Mauricio, Roso Luis, Cascales Concepción, Zaldo Carlos
Opt Express. 2015 May 4;23(9):11135-40. doi: 10.1364/OE.23.011135.
We report the first pulsed laser operation of an Indium-modified Yb:KY(WO4)2 crystal. Indium incorporation enlarges the broadening of the Yb3+ optical bands, reduces crystal lattice parameters and increases n(p) refractive index. A KY0.8In0.07Yb0.13(WO4)2 crystal pumped at 981 nm with a Ti-sapphire laser in a SESAM modulated resonator produces at 300 K self-starting and stable mode-locking. The shortest laser pulses achieved were centred at λ = 1041.1 nm, have a duration of 96 fs with average power of 134 mW and repetition rate of 103.5 MHz (1.3 nJ/pulse).
我们报道了铟改性的Yb:KY(WO4)2晶体的首次脉冲激光运转。掺入铟扩大了Yb3+光学能带的展宽,减小了晶格参数并提高了n(p)折射率。在SESAM锁模谐振腔中,用钛宝石激光器在981 nm泵浦的KY0.8In0.07Yb0.13(WO4)2晶体在300 K时实现了自启动且稳定的锁模。获得的最短激光脉冲中心波长为λ = 1041.1 nm,脉宽为96 fs,平均功率为134 mW,重复频率为103.5 MHz(1.3 nJ/脉冲)。