Nojiri Kie, Tsujimoto Akimasa, Suzuki Takayuki, Shibasaki Syo, Matsuyoshi Saki, Takamizawa Toshiki, Miyazaki Masashi
Department of Operative Dentistry, Nihon University School of Dentistry.
Dent Mater J. 2015;34(5):611-7. doi: 10.4012/dmj.2015-045.
In this study, we investigated the influence of light intensity on the surface-free energy and dentin bond strength of single-step selfetch adhesives. The adhesives were applied to the dentin surfaces of bovine mandibular incisors and cured with light intensities of 0 (no irradiation), 200, 400, and 600 mW/cm(2). Surface-free energies were determined by measuring the contact angles of three test liquids placed on the cured adhesives. Dentin bond strengths of the specimens were also measured. Polymerization with a higher light intensity resulted in a lower surface-free energy of the cured adhesives. The greatest bond strength was achieved when a light intensity of 400 mW/cm(2) or greater was used. Our data suggest that the surface-free energy and dentin bond strength of single-step self-etch adhesives are affected by light intensity of the curing unit.
在本研究中,我们调查了光强度对单步自酸蚀粘结剂的表面自由能和牙本质粘结强度的影响。将粘结剂应用于牛下颌切牙的牙本质表面,并用0(无照射)、200、400和600 mW/cm²的光强度进行固化。通过测量放置在固化粘结剂上的三种测试液体的接触角来测定表面自由能。还测量了标本的牙本质粘结强度。较高光强度的聚合导致固化粘结剂的表面自由能较低。当使用400 mW/cm²或更高的光强度时,可获得最大粘结强度。我们的数据表明,单步自酸蚀粘结剂的表面自由能和牙本质粘结强度受固化单元光强度的影响。