To describe the behavior of 45 discs of dental amalgam of known dimension prepared from three commercially available brands of dental amalgam (Contour® Kerr®-USA, Admix® SDI®-Australia and Nu Alloy® Newstethic®-Colombia) when subjected to the action of high temperatures (200 °C, 400 °C, 600 °C, 800 °C, 1000 °C). It was hoped to establish parameters that could be used for human dental identification in cases of charred, burned or incinerated human remains.
A pseudo-experimental descriptive in-vitro study was designed to describe the macroscopic physical changes to the surface of 45 discs of pre-prepared amalgam of three commercially available brands exposed to a range of high temperatures.
Characteristic and repetitive physical changes were a noticeable feature of the discs of amalgam of each brand of amalgam subjected to the different temperature ranges. These physical changes included changes in dimensional stability, changes in texture, changes in colour, changes in the appearance of fissures and cracks and changes in the fracture and fragmentation of the sample.
The characteristics of dental amalgam may be of assistance in cases of human identification where charred, burned or incinerated human remains are a feature and where fingerprints or other soft tissue features are unavailable.
描述由三种市售品牌的牙科汞合金(美国Contour® Kerr®、澳大利亚Admix® SDI®和哥伦比亚Nu Alloy® Newstethic®)制备的45个已知尺寸的牙科汞合金圆盘在高温(200℃、400℃、600℃、800℃、1000℃)作用下的行为。希望建立可用于在烧焦、烧伤或焚烧的人类遗骸案件中进行人类牙齿鉴定的参数。
设计了一项伪实验性描述性体外研究,以描述三种市售品牌的预制备汞合金的45个圆盘暴露于一系列高温下其表面的宏观物理变化。
在不同温度范围内,每个品牌汞合金圆盘都出现了特征性且重复性的物理变化。这些物理变化包括尺寸稳定性变化、质地变化、颜色变化、裂缝和裂纹外观变化以及样品的断裂和破碎变化。
在烧焦、烧伤或焚烧的人类遗骸是特征且无法获取指纹或其他软组织特征的人类鉴定案件中,牙科汞合金的特性可能会有所帮助。