Effect of Cellulases and Xylanases on Refining Process and Kraft Pulp Properties.

作者信息

Przybysz Buzała Kamila, Przybysz Piotr, Kalinowska Halina, Derkowska Małgorzata

机构信息

Institute of Papermaking and Printing Technology, Lodz University of Technology, Wolczanska str. 223, 90-924, Lodz, Poland.

Institute of Technical Biochemistry, Lodz University of Technology, Stefanowskiego str. 4/10, 90-924, Lodz, Poland.

出版信息

PLoS One. 2016 Aug 24;11(8):e0161575. doi: 10.1371/journal.pone.0161575. eCollection 2016.

Abstract

Samples of bleached kraft pine cellulosic pulp, either treated with an enzyme preparation (a Thermomyces lanuginosus xylanase, an Aspergillus sp. cellulase, and a multienzyme preparation NS-22086 containing both these activities) or untreated, were refined in a laboratory PFI mill. The treatment with cellulases contained in the last two preparations significantly improved the pulp's susceptibility to refining (the target freeness value of 30°SR was achieved in a significantly shorter time), increased water retention value (WRV) and fines contents while the weighted average fiber length was significantly reduced. These changes of pulp parameters caused deterioration of paper strength properties. The treatment with the xylanase, which partially hydrolyzed xylan, small amounts of which are associated with cellulose fibers, only slightly loosened the structure of fibers. These subtle changes positively affected the susceptibility of the pulp to refining (refining energy was significantly reduced) and improved the static strength properties of paper. Thus, the treatment of kraft pulps with xylanases may lead to substantial savings of refining energy without negative effects on paper characteristics.

摘要

对经过酶制剂处理(一种嗜热栖热菌木聚糖酶、一种曲霉属纤维素酶以及包含这两种活性的复合酶制剂NS - 22086)或未处理的漂白硫酸盐松木纤维素浆样品,在实验室PFI磨中进行打浆。后两种制剂中含有的纤维素酶处理显著提高了纸浆的打浆易磨性(在显著更短的时间内达到了30°SR的目标游离度值),增加了保水值(WRV)和细小组分含量,同时加权平均纤维长度显著降低。纸浆参数的这些变化导致纸张强度性能变差。木聚糖酶处理可部分水解与纤维素纤维相关的少量木聚糖,只会使纤维结构稍有松散。这些细微变化对纸浆的打浆易磨性产生了积极影响(打浆能耗显著降低),并改善了纸张的静态强度性能。因此,用木聚糖酶处理硫酸盐浆可大幅节省打浆能耗,且不会对纸张特性产生负面影响。