Abstract
  1. With the finishing agents tested Concise had a smoother surface texture than Aspa. 2. The smoothest surface was on Concise polymerized against a Mylar matrix strip. The smoothest surface for Aspa was obtained with a silicon carbide disk. 3. Aspa abraded about three times as rapidly by volume as Concise when tested by a two-body abrasion method. 4. Significantly more air bubbles were entrapped by hand mixing within Aspa than within Concise. 5. Controlled clinical studies of the glass-ionomer cements are needed before they can be fully evaluated as restorative materials.
摘要
  1. 在所测试的处理剂中,Concise的表面质地比Aspa更光滑。2. 当与聚酯薄膜基质条聚合时,Concise的表面最光滑。Aspa最光滑的表面是用碳化硅盘获得的。3. 通过双体磨损法测试时,Aspa的磨损体积约为Concise的三倍。4. 手工搅拌时,Aspa中截留的气泡明显多于Concise。5. 在将玻璃离子水门汀作为修复材料进行全面评估之前,需要进行对照临床研究。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验