Department of Bio-fibers and Materials Science, Kyungpook National University, Daegu 41566, Republic of Korea.
Department of Biosystems & Biomaterials Science and Engineering, Seoul National University, Seoul 08826, Republic of Korea.
Int J Biol Macromol. 2017 Nov;104(Pt A):294-302. doi: 10.1016/j.ijbiomac.2017.06.019. Epub 2017 Jun 7.
In the present study, the effects of different degumming methods on the structural characteristics and properties of regenerated silk fibroin (SF) were examined. The crystallinity index of the degummed silk increased with the degumming ratio. The crystallinity index at any given degumming ratio differed depending on the degumming method. The soda method and the soap/soda method using sodium carbonate resulted in a higher crystallinity index than the other methods The degumming method strongly affects the molecular weight (MW) and solution viscosity of the regenerated SF. The MW and viscosity of the regenerated SF, according to the degumming method, was in the order of urea method>HTHP method≈acid method>soap/soda method≈soda method. The turbidity of a silk formic acid solution decreased as a result of increasing the degumming ratio and was a minimum at a degumming ratio of around 26%. However, it was not affected by the degumming method. The mechanical properties of a regenerated SF film were strongly affected by the degumming method and the trend in the strength and elongation with the various degumming methods was the same as that of the MW and viscosity of the regenerated SF.
本研究考察了不同脱胶方法对再生丝素纤维(SF)结构特性和性能的影响。脱胶后丝的结晶度指数随脱胶率的增加而增加。在任何给定的脱胶率下,结晶度指数因脱胶方法而异。苏打法和使用碳酸钠的皂/苏打法的结晶度指数均高于其他方法。脱胶方法强烈影响再生 SF 的分子量(MW)和溶液粘度。根据脱胶方法,再生 SF 的 MW 和粘度的顺序为尿素法>HTHP 法≈酸法>皂/苏打法≈苏打法。丝甲酸溶液的浊度随脱胶率的增加而降低,在脱胶率约为 26%时达到最低。然而,它不受脱胶方法的影响。再生 SF 薄膜的机械性能受脱胶方法的强烈影响,各种脱胶方法的强度和伸长率的趋势与再生 SF 的 MW 和粘度相同。