Patel Mitesh, Stopher Miles A
Department of Physics, Imperial College London, London, UK
Department of Materials Science and Metallurgy, University of Cambridge, Cambridge, UK.
Philos Trans A Math Phys Eng Sci. 2017 Jul 28;375(2098). doi: 10.1098/rsta.2017.0030.
This is a transcript of the discussion session on the effects of hydrogen in the non-ferrous alloys of zirconium and titanium, which are anisotropic hydride-forming metals. The four talks focus on the hydrogen embrittlement mechanisms that affect zirconium and titanium components, which are respectively used in the nuclear and aerospace industries. Two specific mechanisms are delayed hydride cracking and stress corrosion cracking.This article is part of the themed issue 'The challenges of hydrogen and metals'.
这是关于氢对锆和钛的有色金属合金影响的讨论环节文字记录,锆和钛是形成各向异性氢化物的金属。四场报告聚焦于影响锆和钛部件的氢脆化机制,这两种金属分别应用于核工业和航空航天工业。两种具体机制是延迟氢化物开裂和应力腐蚀开裂。本文是主题为“氢与金属的挑战”特刊的一部分。