Suppr超能文献

445纳米二极管激光辅助拆除自锁陶瓷托槽对剪切粘结强度的影响

Effects of 445-nm Diode Laser-Assisted Debonding of Self-Ligating Ceramic Brackets on Shear Bond Strength.

作者信息

Stein Steffen, Hellak Andreas, Schauseil Michael, Korbmacher-Steiner Heike, Braun Andreas

机构信息

1 Department of Orthodontics, University of Marburg , Marburg, Germany .

2 Department of Operative Dentistry and Endodontology, University of Marburg , Marburg, Germany .

出版信息

Photomed Laser Surg. 2018 Jan;36(1):31-36. doi: 10.1089/pho.2017.4314. Epub 2017 Oct 10.

Abstract

OBJECTIVE

The aim of this study was to measure the effect of irradiation with a novel 445-nm diode laser on the shear bond strength (SBS) of ceramic brackets before debonding.

MATERIALS AND METHODS

Thirty ceramic brackets (In-Ovation C, GAC) were bonded in standard manner to the planed and polished buccal enamel surfaces of 30 caries-free human third molars. Each tooth was randomly allocated to the laser or control group, with 15 samples per group. The brackets in the laser group were irradiated with the diode laser (SIROLaser Blue; Sirona) on three sides of the bracket bases for 5 sec each (lateral-coronal-lateral, a total of 15 sec) immediately before debonding. SBS values were measured for the laser group and control group. To assess the adhesive remnant index (ARI) and the degree of enamel fractures, micrographs of the enamel surface were taken with 10-fold magnification after debonding.

RESULTS

The SBS values were significantly lower statistically in the laser group in comparison with the control group (p < 0.05). The ARI scores were also significantly lower statistically in the laser group in comparison with the control group (p < 0.05). No bracket fractures or enamel fractures occurred in either group after debonding.

CONCLUSIONS

Irradiation of ceramic brackets with the novel diode laser before debonding significantly reduces the SBS values. This is of clinical importance, as it means that the risk of damage to the teeth, bracket fractures, and the overall treatment time can be reduced.

摘要

目的

本研究的目的是测量新型445纳米二极管激光照射对陶瓷托槽在脱粘前的剪切粘结强度(SBS)的影响。

材料与方法

将30个陶瓷托槽(In-Ovation C,GAC)以标准方式粘结到30颗无龋人类第三磨牙的经平面处理和抛光的颊面釉质表面。每颗牙齿随机分配到激光组或对照组,每组15个样本。在脱粘前,立即用二极管激光(SIROLaser Blue;西诺德)对激光组托槽底座的三个侧面各照射5秒(侧面-冠部-侧面,共15秒)。测量激光组和对照组的SBS值。为了评估粘结剂残留指数(ARI)和釉质骨折程度,在脱粘后用10倍放大倍数拍摄釉质表面的显微照片。

结果

与对照组相比,激光组的SBS值在统计学上显著更低(p < 0.05)。与对照组相比,激光组的ARI评分在统计学上也显著更低(p < 0.05)。脱粘后两组均未发生托槽骨折或釉质骨折。

结论

在脱粘前用新型二极管激光照射陶瓷托槽会显著降低SBS值。这具有临床重要性,因为这意味着可以降低牙齿损伤、托槽骨折的风险以及总体治疗时间。