Suppr超能文献

CAD/CAM聚合材料对乳磨牙磨损的体外研究

In Vitro Investigation of Wear of CAD/CAM Polymeric Materials Against Primary Teeth.

作者信息

Choi Jae-Won, Song Eun-Ju, Shin Jong-Hyun, Jeong Tae-Sung, Huh Jung-Bo

机构信息

Department of Prosthodontics, Dental Research Institute, Institute of Translational Dental Sciences, BK21 PLUS Project, School of Dentistry, Pusan National University, Yangsan 50612, Korea.

Department of Pediatric Dentistry, School of Dentistry, Pusan National University, Yangsan 50612, Korea.

出版信息

Materials (Basel). 2017 Dec 9;10(12):1410. doi: 10.3390/ma10121410.

Abstract

The aim of the study was to evaluate the effects of polymeric computer-aided design/computer-aided manufacturing CAD/CAM materials on antagonistic primary tooth wear. Five CAD/CAM polymeric materials were examined: Vipi Block Monocolor (VBM), Yamahachi polymethylmethacrylate (PMMA) (YAP), Mazic Duro (MZD), Vita Enamic (ENA), and Pekkton (PEK). All of the specimens were tested in a thermomechanical loading machine with the primary canine as the antagonist (50 N, 1.2 × 10⁵ cycles, 1.7 Hz, 5/55 °C). The wear losses of the antagonist tooth and the restorative materials were calculated using reverse modelling software and an electronic scale. VBM and ENA showed significantly higher antagonist tooth wear than PEK ( < 0.05), but there was no significant difference observed among VBM, YAP, MZD, and ENA ( > 0.05). PEK showed the largest value in both material volumetric and weight losses. In terms of material volumetric losses, there was no significant difference between all of the groups ( > 0.05). In terms of material weight losses, PEK was significantly larger than ENA ( < 0.05), but there was no significant difference between VBM, YAP, MZD, and ENA ( > 0.05). Volumetric and weight losses of materials showed similar wear behaviour. However, the wear patterns of antagonists and materials were different, especially in PEK.

摘要

本研究的目的是评估聚合物计算机辅助设计/计算机辅助制造(CAD/CAM)材料对拮抗乳牙磨损的影响。研究了五种CAD/CAM聚合物材料:Vipi Block Monocolor(VBM)、Yamahachi聚甲基丙烯酸甲酯(PMMA)(YAP)、Mazic Duro(MZD)、Vita Enamic(ENA)和Pekkton(PEK)。所有标本均在热机械加载机中以乳尖牙作为拮抗剂进行测试(50 N,1.2×10⁵次循环,1.7 Hz,5/55°C)。使用逆向建模软件和电子天平计算拮抗牙和修复材料的磨损损失。VBM和ENA的拮抗牙磨损明显高于PEK(<0.05),但VBM、YAP、MZD和ENA之间未观察到显著差异(>0.05)。PEK在材料体积损失和重量损失方面均显示出最大值。在材料体积损失方面,所有组之间均无显著差异(>0.05)。在材料重量损失方面,PEK明显大于ENA(<0.05),但VBM、YAP、MZD和ENA之间无显著差异(>0.05)。材料的体积损失和重量损失表现出相似的磨损行为。然而,拮抗牙和材料的磨损模式不同,尤其是在PEK中。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/a94e/5744345/b96936c19685/materials-10-01410-g002.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验