Department of Dental Materials and Prosthodontics, Aracatuba Dental School, UNESP - Univ Estadual Paulista, Campus of Aracatuba, Sao Paulo, Brazil.
J Prosthodont. 2018 Aug;27(7):624-635. doi: 10.1111/jopr.12727. Epub 2017 Dec 13.
The objective of this systematic review with meta-analysis was to evaluate surface treatment in yttria-stabilized tetragonal zirconia polycrystal ceramic (Y-TZP) on the shear bond strength (SBS) values between Y-TZP (core ceramic) and veneer ceramic, compared to untreated specimens.
This review was registered at PROSPERO platform under the number CRD42016036493. The systematic review of the extracted publications was performed to compare the effect of surface treatment on SBS between Y-TZP ceramic and veneering ceramic. A comprehensive review of the literature from the earliest available dates through January 2017 was performed in the PubMed/Medline, Embase, Scopus, and Cochrane Library databases.
A total of 15 studies were identified for the inclusion of data, with only in vitro studies. A random-effect model found statistically significant differences between untreated and treated surfaces of Y-TZP (p < 0.00001; MD: 2.84; 95% CI: 2.19 to 3.49). In another analysis, a random-effect model found statistically significant differences between the groups that only performed the associations of treatments and control group (p < 0.00001; MD: 3.19; 95% CI: 2.11 to 4.28).
Surface treatment in Y-TZP improved the values of SBS between the Y-TZP and veneer ceramic. The associations between two or more treatments also showed positive effect on the bond strength due the cumulative effect of the treatments.
本系统评价和荟萃分析的目的是评估钇稳定四方氧化锆多晶陶瓷(Y-TZP)的表面处理对 Y-TZP(核心陶瓷)和贴面陶瓷之间的剪切结合强度(SBS)值的影响,与未处理的标本相比。
本综述在 PROSPERO 平台上进行,编号为 CRD42016036493。对提取的文献进行系统评价,以比较表面处理对 Y-TZP 陶瓷和贴面陶瓷之间 SBS 的影响。通过 PubMed/Medline、Embase、Scopus 和 Cochrane Library 数据库对最早可获得日期至 2017 年 1 月的文献进行全面综述。
共确定了 15 项研究纳入数据,均为体外研究。随机效应模型发现 Y-TZP 未处理和处理表面之间存在统计学上显著差异(p<0.00001;MD:2.84;95%CI:2.19 至 3.49)。在另一项分析中,随机效应模型发现仅进行处理联合与对照组之间的组间存在统计学上显著差异(p<0.00001;MD:3.19;95%CI:2.11 至 4.28)。
Y-TZP 的表面处理提高了 Y-TZP 和贴面陶瓷之间 SBS 的值。由于处理的累积效应,两种或更多种处理之间的联合也对结合强度产生了积极影响。