The aim of this study was to evaluate the influence of dentin pretreatment with NaOCl on shear bond strength of four one-step self-etch adhesives with different pH values.
Bovine permanent incisors were used. Four one-step self-etch adhesives were tested: Adper™ Easy Bond, Futurabond NR, G-aenial Bond, Clearfil S3 Bond. One two-step self-etch adhesive (Clearfil SE Bond) was used as control. Group 1- no pretreatment; group 2- pretratment with 5,25 % NaOCl; group 3- pretreatment with 37 % H3PO4 etching and 5,25 % NaOCl. A hybrid composite resin was inserted into the dentin surface. The specimens were tested in a universal testing machine. The examiners evaluated the fractured surfaces in optical microscope to determine failure modes, quantified with adhesive remnant index (ARI).
Dentin pretreatment variably influenced bond strength values of the different adhesive systems. When no dentin pretreatment was applied, no significant differences were found ( >.05) among four adhesives tested. No significant differences were recorded when comparing NaOCl pretreatment with H3PO4 + NaOCl pretreatment for all adhesive tested ( >.05) except Clearfil S3 Bond that showed higher shear bond strength values when H3PO4 was applied. Frequencies of ARI scores were calculated.
The influence of dentin pretreatment with NaOCl depends on the composition of each adhesive system used. There was no difference in bond strength values among self-etch adhesives with different pH values. Dentin, pretreatment, self-etch adhesives.
本研究旨在评估用次氯酸钠(NaOCl)对牙本质进行预处理,对四种不同pH值的一步法自酸蚀粘结剂的剪切粘结强度的影响。
使用牛恒切牙。测试了四种一步法自酸蚀粘结剂:Adper™ Easy Bond、Futurabond NR、G-aenial Bond、Clearfil S3 Bond。使用一种两步法自酸蚀粘结剂(Clearfil SE Bond)作为对照。第1组 - 不进行预处理;第2组 - 用5.25%的NaOCl进行预处理;第3组 - 用37%的磷酸(H3PO4)酸蚀并结合5.25%的NaOCl进行预处理。将一种混合复合树脂充填到牙本质表面。在万能试验机上对标本进行测试。检查人员在光学显微镜下评估断裂面以确定失败模式,并用粘结剂残留指数(ARI)进行量化。
牙本质预处理对不同粘结剂系统的粘结强度值有不同程度的影响。当不进行牙本质预处理时,在所测试的四种粘结剂之间未发现显著差异(P>.05)。对于所有测试的粘结剂,将NaOCl预处理与H3PO4 + NaOCl预处理进行比较时,除了Clearfil S3 Bond在使用H3PO4时显示出更高的剪切粘结强度值外,均未记录到显著差异(P>.05)。计算了ARI评分的频率。
用NaOCl对牙本质进行预处理的影响取决于所使用的每种粘结剂系统的组成。不同pH值的自酸蚀粘结剂之间的粘结强度值没有差异。牙本质、预处理、自酸蚀粘结剂。