Suppr超能文献

正畸间接粘结树脂的比较:一项前瞻性研究。

and comparison of orthodontic indirect bonding resins: A prospective study.

作者信息

Pamukcu H, Ozsoy O Polat, Dagalp R

机构信息

Department of Orthodontics, Faculty of Dentistry, Baskent University, Ankara, Turkey.

Private Practice, Ankara University, Ankara, Turkey.

出版信息

Niger J Clin Pract. 2018 May;21(5):614-623. doi: 10.4103/njcp.njcp_252_17.

Abstract

OBJECTIVE

The aim of this study was to evaluate in vitro shear bond strength (SBS) and in vivo bond survival rates of brackets bonded using orthodontic indirect bonding resins.

MATERIALS AND METHODS

For the in vitro study, the first group was direct bonding control group. In Groups II and III, bonding was performed with indirect bonding resins that were either chemically or light-cured. The SBS of each sample was examined. For the in vivo study, full-mouth brackets were placed in 20 patients using a split-mouth approach, with either chemically-cured or a light-cured indirect bonding resin. The patients were followed for 12 months. Data were statistically evaluated using analysis of variance, Tukey's tests, and Weibull survival analysis.

RESULTS

The mean SBS values (MPa) were 17.6 ± 6.6, 13.1 ± 4.7, and 15.1 ± 5.9 for Group I, Groups II, and III, respectively, (P < 0.05). The adhesive remnant index scores of the groups were generally Score 3 and Score 4. In vivo follow-up showed no statistically significant differences in total bond failure rate between groups (P > 0.05).

CONCLUSIONS

In vitro study showed lower SBS with chemically-cured indirect bonding resin than flowable light-cured resin and the control group, but in vivo failure rates of both indirect resins were found to be adequate for clinical usage.

摘要

目的

本研究旨在评估使用正畸间接粘结树脂粘结的托槽的体外剪切粘结强度(SBS)和体内粘结存留率。

材料与方法

在体外研究中,第一组为直接粘结对照组。在第二组和第三组中,使用化学固化或光固化的间接粘结树脂进行粘结。检测每个样本的SBS。在体内研究中,采用双侧对照法为20例患者全口放置托槽,分别使用化学固化或光固化间接粘结树脂。对患者进行12个月的随访。使用方差分析、Tukey检验和威布尔生存分析对数据进行统计学评估。

结果

第一组、第二组和第三组的平均SBS值(MPa)分别为17.6±6.6、13.1±4.7和15.1±5.9(P<0.05)。各组的粘结剂残留指数评分大多为3分和4分。体内随访显示,各组之间的总粘结失败率无统计学显著差异(P>0.05)。

结论

体外研究表明,化学固化间接粘结树脂的SBS低于可流动光固化树脂和对照组,但两种间接树脂的体内失败率在临床上均适用。