Suppr超能文献

傅里叶变换红外光谱法/衰减全反射分析法用于检测Transbond XT粘接剂系统的固化程度和剪切粘结强度

Fourier-transform infrared spectroscopy/attenuated total reflectance analysis for the degree of conversion and shear bond strength of Transbond XT adhesive system.

作者信息

Masood Taha Mohammed, Abbassy Mona Aly, Bakry Ahmed Samir, Matar Naof Yessen, Hassan Ali Habib

机构信息

Dental and Maxillofacial Department, Saudi German Hospital, Jeddah, Saudi Arabia.

Orthodontics Department, Faculty of Dentistry, Batterjee Medical College, Jeddah, Saudi Arabia.

出版信息

Clin Cosmet Investig Dent. 2018 Dec 7;10:275-280. doi: 10.2147/CCIDE.S169438. eCollection 2018.

Abstract

OBJECTIVE

The objectives of this study were to evaluate the degree of conversion (DC) for Transbond XT curing light of intensity 1,600 mW/cm by using variable curing durations and to determine the effect of the tested curing durations adopted in the current experiment on shear bond strength of Transbond XT resin cement.

MATERIALS AND METHODS

A total of 85 orthodontic ceramic brackets (Victory series; 3M Unitek) were utilized in the current experiment. The bonding system used in the current study was Transbond XT Primer followed by Transbond PLUS Color Change Adhesive (3M Unitek) that cured for 3, 6, and 9 seconds. The method was done by polymerization of the adhesive under a ceramic bracket for 40 ceramic brackets. The other 45 brackets were divided into three groups (n=15) according to the curing time duration (3, 6, and 9 seconds). The bonded specimens in each group were debonded using a shear load applied at the bracket bases by the blades of an Instron universal testing machine (ElectroPlus E1000; Instron) and directed in an occlusogingival direction with a crosshead speed of 0.5 mm/min utilizing 50 kg load cell.

RESULTS

One-way ANOVA revealed that 6 and 9 seconds curing by the Ortholux light cure scored significantly higher values when compared to the 3 seconds curing.

CONCLUSION

Curing the Transbond XT for 6 and 9 seconds recorded a significant improvement of bond strength and DC.

摘要

目的

本研究的目的是通过使用不同的固化时间来评估强度为1600 mW/cm的Transbond XT固化灯的转化率(DC),并确定当前实验中采用的测试固化时间对Transbond XT树脂水门汀剪切粘结强度的影响。

材料与方法

本实验共使用了85个正畸陶瓷托槽(Victory系列;3M Unitek)。本研究中使用的粘结系统是Transbond XT底漆,随后是Transbond PLUS变色粘合剂(3M Unitek),固化时间分别为3秒、6秒和9秒。该方法是在40个陶瓷托槽下对粘合剂进行聚合。根据固化时间(3秒、6秒和9秒)将另外45个托槽分为三组(n = 15)。每组中的粘结标本使用Instron万能试验机(ElectroPlus E1000;Instron)的刀片在托槽底部施加剪切载荷进行脱粘,并利用50 kg测力传感器以0.5 mm/min的十字头速度沿咬合龈向方向进行。

结果

单因素方差分析显示,与3秒固化相比,Ortholux光固化6秒和9秒时的值显著更高。

结论

Transbond XT固化6秒和9秒时,粘结强度和转化率有显著提高。