Dhara Palash, Bhandaru Nandini, Das Anuja, Mukherjee Rabibrata
Instability and Soft Patterning Laboratory, Department of Chemical Engineering, Indian Institute of Technology Kharagpur, Kharagpur, Pin-721302, India.
Sci Rep. 2018 May 8;8(1):7169. doi: 10.1038/s41598-018-25504-7.
Spin dewetting refers to spontaneous rupture of the dispensed solution layer during spin coating, resulting in isolated but periodic, regular sized domains of the solute and is pre-dominant when the solute concentration (C ) is very low. In this article we report how the morphology of liquid crystal (LC) 5CB thin films coated on flat and patterned PMMA substrate transform from spin dewetted droplets to continuous films with increase in C . We further show that within the spin dewetted regime, with gradual increase in the solute concentration, periodicity of the isotropic droplets (λ ) as well as their mean diameter (d ), gradually decreases, till the film becomes continuous at a critical concentration (C *). Interestingly, the trend that λ reduces with increase in C is exact opposite to what is observed in thermal/solvent vapor induced dewetting of a thin film. The spin dewetted droplets exhibit transient Radial texture, in contrast to Schlieren texture observed in elongated threads and continuous films of 5CB, which remains in the Nematic phase at room temperature. Finally we show that by casting the film on a grating patterned substrate it becomes possible to align the spin dewetted droplets along the contours substrate patterns.
旋转去湿是指在旋涂过程中所分配溶液层的自发破裂,导致溶质形成孤立但周期性、规则尺寸的区域,并且当溶质浓度(C )非常低时占主导地位。在本文中,我们报道了涂覆在平坦和图案化聚甲基丙烯酸甲酯(PMMA)衬底上的液晶(LC)5CB薄膜的形态如何随着C 的增加从旋转去湿的液滴转变为连续薄膜。我们进一步表明,在旋转去湿状态下,随着溶质浓度逐渐增加,各向同性液滴的周期性(λ )及其平均直径(d )逐渐减小,直到在临界浓度(C *)时薄膜变为连续。有趣的是,λ 随C 增加而减小的趋势与在热/溶剂蒸汽诱导的薄膜去湿中观察到的情况完全相反。旋转去湿的液滴呈现瞬态径向纹理,这与在5CB的细长线和连续薄膜中观察到的纹影纹理相反,5CB在室温下处于向列相。最后我们表明,通过在光栅图案化衬底上浇铸薄膜,可以使旋转去湿的液滴沿着衬底图案的轮廓排列。