含氟磷灰石和羟基磷灰石的玻璃离子水门汀的氟释放

Fluoride Release From Glass Ionomer Cement Containing Fluoroapatite And Hydroxyapatite.

作者信息

Malik Sofia, Ahmed Muhammad Adeel, Choudhry Ziaullah, Mughal Nouman, Amin Muhammad, Lone Muneeb Ahmed

机构信息

Dow University of Health Sciences, Karachi, Pakistan.

出版信息

J Ayub Med Coll Abbottabad. 2018 Apr-Jun;30(2):198-202.

Abstract

BACKGROUND

Many investigators reported the amount of fluoride release from glass ionomer cement. However, the work on fluoride release from GIC containing fluoroapatite and hydroxyapatite is scarce. Therefore, this study was conducted to find out the amount of fluoride release from Glass ionomer cement containing fluoroapatite and hydroxyapatite.

METHODS

The study was conducted in the Department of Materials, Queen Marry University of London. A total of 108 samples equally divided in to three groups namely fluoroapatite added GIC, Hydroxyapatite added GIC as an experimental group and unmodified GIC as a control group. The specimens were prepared by mixing powder and liquid in the ratio of 1:1. Amount of fluoride released was measured by Ion electrode method at 1, 3, 7, 14, 21 and 28 days.

RESULTS

On day 1, the combination of FA +GIC showed the highest amount of fluoride release followed by the control group (GIC) whereas the combination of HA+GIC released the least amount of fluoride. On day 7, the amount of fluoride release started declining in all three groups. The amount of fluoride release continued decreasing on day 21 in which combination of FA +GIC and the control group are shown to release equal amount of fluoride whereas the combination of HA+GIC gave the least activity the amount of fluoride release fall to a minimum level in all three group by day 28.

CONCLUSIONS

It is concluded that addition of fluoroapatite into GIC has significant effect on the amount of fluoride release as compared to GIC alone; however, addition of hydroxyapatite into GIC has no additive effect on the amount of fluoride release.

摘要

背景

许多研究人员报告了玻璃离子水门汀释放氟化物的量。然而,关于含氟磷灰石和羟基磷灰石的玻璃离子水门汀释放氟化物的研究较少。因此,本研究旨在确定含氟磷灰石和羟基磷灰石的玻璃离子水门汀释放氟化物的量。

方法

该研究在伦敦玛丽女王大学材料系进行。总共108个样本平均分为三组,即添加氟磷灰石的玻璃离子水门汀组、添加羟基磷灰石的玻璃离子水门汀组作为实验组,以及未改性的玻璃离子水门汀组作为对照组。通过将粉末和液体按1:1的比例混合来制备标本。在第1、3、7、14、21和28天,采用离子电极法测量氟化物释放量。

结果

在第1天,氟磷灰石+玻璃离子水门汀组合显示出最高的氟化物释放量,其次是对照组(玻璃离子水门汀),而羟基磷灰石+玻璃离子水门汀组合释放的氟化物量最少。在第7天,所有三组的氟化物释放量开始下降。在第21天,氟化物释放量继续下降,其中氟磷灰石+玻璃离子水门汀组合和对照组释放的氟化物量相等,而羟基磷灰石+玻璃离子水门汀组合的活性最低。到第28天,所有三组的氟化物释放量均降至最低水平。

结论

得出的结论是,与单独的玻璃离子水门汀相比,向玻璃离子水门汀中添加氟磷灰石对氟化物释放量有显著影响;然而,向玻璃离子水门汀中添加羟基磷灰石对氟化物释放量没有累加效应。