Polyethylenimine (PEI) functionalized kaolinite clay was successfully prepared, characterized, and assessed for the remediation of volatile organic compounds (VOCs) comprising the aldehyde, carboxylic acid, and disulfide functional group classes. A gas chromatographic vapor capture assay evaluated the capability of unmodified and modified clay material to capture representative aldehyde, carboxylic acid, and disulfide VOCs in a laboratory setting. Unmodified kaolinite (Kao) clay was moderately or poorly effective at remediating these VOCs, while the poly(amine) functionalized Kao was capable of capturing VOCs in the vapor phase with reductions up to 100%. Sample cartridge tubes were packed with PEI-functionalized clay in order to assess their ability to reduce the detectable volatile fatty acid load at an open-air rendering plant in a relevant field test for applying these materials in a packed-bed scrubber application. The PEI-Kao packed cartridges were capable of significantly reducing the detectable concentration of volatile fatty acid effluent from the rendering operation. These volatile fatty acids are major contributors to nuisance odors associated with rendering.
成功制备了聚乙烯亚胺(PEI)功能化高岭土,并对其进行了表征,用于修复包含醛、羧酸和二硫化物官能团类别的挥发性有机化合物(VOCs)。气相色谱蒸气捕集测定法评估了未改性和改性粘土材料在实验室环境中捕获代表性醛、羧酸和二硫化物 VOC 的能力。未改性高岭土(Kao)粘土对这些 VOC 的修复效果中等或较差,而聚(胺)功能化 Kao 能够以高达 100%的比例捕获蒸气相中的 VOC。为了评估它们在相关现场测试中在填充床洗涤器应用中应用这些材料的能力,将 PEI 功能化粘土填充到样品盒管中,以减少露天炼油厂中可检测挥发性脂肪酸负荷。PEI-Kao 填充盒管能够显著降低炼油操作中挥发性脂肪酸流出物的可检测浓度。这些挥发性脂肪酸是与炼油相关的异味的主要贡献者。