Suppr超能文献

掺加早强水泥的再生骨料混凝土蒸汽养护制度优化——参数研究

Optimization of Steam-Curing Regime for Recycled Aggregate Concrete Incorporating High Early Strength Cement-A Parametric Study.

作者信息

Hanif Asad, Kim Yongjae, Usman Muhammad, Park Cheolwoo

机构信息

Department of Civil Engineering, Mirpur University of Science and Technology (MUST), Allama Iqbal Road, Mirpur AJ&K 10250, Pakistan.

Department of Civil Engineering, Kangwon National University, 346, Jungang-ro, Samcheok-si, Gangwon-do 25913, Korea.

出版信息

Materials (Basel). 2018 Dec 7;11(12):2487. doi: 10.3390/ma11122487.

Abstract

This paper investigates the properties of steam cured recycled aggregate concrete (RAC), in an attempt to determine the optimum conditions of the steam-curing cycle for RAC, and incorporating high early strength cement (HESC). Varying conditions of steam curing were employed. The steam-curing cycle was set based on the peak temperature, and the duration for which the peak temperature was maintained. Three peak temperatures were used for steam curing, 50 °C, 60 °C, and 70 °C, maintained for up to two hours. The compressive strength results indicated that the steam-curing cycle employing the peak temperature of 50 °C maintained for one hour with a total duration of four hours was the optimum for strength development, both at the early and late stages of hydration. Determining the optimum steam-curing temperature and duration will help reduce the associated curing cost, thus further economizing the production cost of recycled aggregate concrete.

摘要

本文研究了蒸汽养护再生骨料混凝土(RAC)的性能,旨在确定RAC蒸汽养护周期的最佳条件,并掺入高早强水泥(HESC)。采用了不同的蒸汽养护条件。蒸汽养护周期根据峰值温度以及保持峰值温度的持续时间来设定。蒸汽养护使用了三个峰值温度,50℃、60℃和70℃,并保持长达两小时。抗压强度结果表明,峰值温度为50℃、保持一小时且总时长为四小时的蒸汽养护周期,对于水化早期和后期的强度发展而言都是最佳的。确定最佳的蒸汽养护温度和持续时间将有助于降低相关的养护成本,从而进一步节约再生骨料混凝土的生产成本。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/e0bb/6316945/23ff11e18c53/materials-11-02487-g001.jpg