Suppr超能文献

研究碘废物形态在稀溶液条件下的耐久性。

Investigating the Durability of Iodine Waste Forms in Dilute Conditions.

作者信息

Asmussen R Matthew, Ryan Joseph V, Matyas Josef, Crum Jarrod V, Reiser Joelle T, Avalos Nancy, McElroy Erin M, Lawter Amanda R, Canfield Nathan C

机构信息

Energy and Environment Directorate, Pacific Northwest National Laboratory, Richland, WA 99352, USA.

出版信息

Materials (Basel). 2019 Feb 26;12(5):686. doi: 10.3390/ma12050686.

Abstract

To prevent the release of radioiodine during the reprocessing of used nuclear fuel or in the management of other wastes, many technologies have been developed for iodine capture. The capture is only part of the challenge as a durable waste form is required to ensure safe disposal of the radioiodine. This work presents the first durability studies in dilute conditions of two AgI-containing waste forms: hot-isostatically pressed silver mordenite (AgZ) and spark plasma sintered silver-functionalized silica aerogel (SFA) iodine waste forms (IWF). Using the single-pass flow-through (SPFT) test method, the dissolution rates respective to Si, Al, Ag and I were measured for variants of the IWFs. By combining solution and solid analysis information on the corrosion mechanism neutral-to-alkaline conditions was elucidated. The AgZ samples were observed to have corrosion preferentially occur at secondary phases with higher Al and alkali content. These phases contained a lower proportion of I compared with the matrix. The SFA samples experienced a higher extent of corrosion at Si-rich particles, but an increased addition of Si to the waste led to an improvement in corrosion resistance. The dissolution rates for the IWF types are of similar magnitude to other Si-based waste form materials measured using SPFT.

摘要

为防止在乏核燃料后处理过程或其他废物管理过程中释放放射性碘,人们已开发出多种碘捕获技术。捕获只是挑战的一部分,因为需要一种耐用的废物形式来确保放射性碘的安全处置。这项工作首次展示了在稀溶液条件下对两种含碘化银废物形式的耐久性研究:热等静压银丝光沸石(AgZ)和放电等离子烧结银功能化二氧化硅气凝胶(SFA)碘废物形式(IWF)。使用单通道流通(SPFT)测试方法,测量了IWF变体中硅、铝、银和碘的溶解速率。通过结合溶液和固体分析信息,阐明了中性至碱性条件下的腐蚀机制。观察到AgZ样品的腐蚀优先发生在铝和碱含量较高的第二相。与基体相比,这些相中碘的比例较低。SFA样品在富硅颗粒处的腐蚀程度更高,但向废物中增加硅的添加量可提高耐腐蚀性。IWF类型的溶解速率与使用SPFT测量的其他硅基废物形式材料的溶解速率大小相似。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/a313/6427718/8ee5f59c8073/materials-12-00686-g001.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验