Oper Dent. 2020 Jan/Feb;45(1):19-29. doi: 10.2341/18-230-C. Epub 2019 Apr 29.
The aim of this prospective, randomized, split-mouth clinical trial was to evaluate postoperative sensitivity, clinical performance, and interproximal contacts after using different restorative systems.
Fifty-three subjects each received three class II restorations according to the restorative systems: conventional resin composite (PA: Peak Universal+Amelogen Plus, Ultradent), low-shrinkage flowable and nanoparticulate resin composites (ABF: Adper Single Bond 2+Filtek Bulk Fill Flow+Filtek Z350XT, 3M ESPE), and low-shrinkage flowable and microhybrid resin composites (XST: XP Bond+SDR+TPH3, Dentsply). Postoperative sensitivity was assessed at 24 hours, seven days, 90 days, and six months. The clinical performance and interproximal contacts were evaluated at baseline, six months, and one year. Friedman, Wilcoxon, Kruskal-Wallis, and Mann-Whitney tests were used to evaluate postoperative sensitivity and interproximal contacts. The equality test of two proportions and logistic regression analysis were used to assess the clinical performance.
No statistically significant differences were observed among groups for postoperative sensitivity. The highest spontaneous sensitivity was reported at 24 hours. ABF was the only group that did not present a reduction in cold sensitivity. Color, marginal discoloration, and superficial staining showed differences among the groups. XST did not show superficial staining after one year. No differences were observed among groups in relation to interproximal contacts. XST resulted in the loss of interproximal contact after one year.
Different types of restorative systems do not influence postoperative sensitivity; however, ABF maintained cold sensitivity over time. Marginal discoloration occurred for all groups but occurred earliest for PA. XST presented a reduction of interproximal contact after one year of evaluation.
本前瞻性、随机、分口临床研究的目的是评估使用不同修复系统后的术后敏感性、临床性能和邻面接触。
53 名受试者每人根据修复系统接受三个 II 类修复体:传统树脂复合材料(PA:Peak Universal+Amelogen Plus,Ultradent)、低收缩流动性和纳米颗粒树脂复合材料(ABF:Adper Single Bond 2+Filtek Bulk Fill Flow+Filtek Z350XT,3M ESPE)以及低收缩流动性和微混合树脂复合材料(XST:XP Bond+SDR+TPH3,Dentsply)。术后敏感性分别在 24 小时、7 天、90 天和 6 个月进行评估。基线、6 个月和 1 年评估临床性能和邻面接触。采用 Friedman、Wilcoxon、Kruskal-Wallis 和 Mann-Whitney 检验评估术后敏感性和邻面接触。采用两比例相等性检验和逻辑回归分析评估临床性能。
各组之间术后敏感性无统计学差异。最高的自发性敏感性报告在 24 小时。ABF 是唯一一组没有冷敏感性降低的组。颜色、边缘变色和表面染色在各组之间存在差异。XST 一年后没有出现表面染色。各组之间邻面接触无差异。XST 一年后导致邻面接触丧失。
不同类型的修复系统不会影响术后敏感性;然而,ABF 随着时间的推移保持冷敏感性。所有组都出现了边缘变色,但最早出现在 PA 组。XST 一年后邻面接触减少。