Rathi Akhil, Pande Neelam, Radke Usha, Deshpande Saee, Chandak Anuj
Department of Prosthodontics, V.S.P.M's Dental College and Research Centre, Nagpur, Maharashtra, India.
J Indian Prosthodont Soc. 2019 Jul-Sep;19(3):248-254. doi: 10.4103/jips.jips_45_19.
This study evaluated and compared the diametral tensile strength (DTS) of phosphate-bonded investment (PBI) material (ringless) used in removable cast partial denture fabrication.
Comparative - study.
The PBI material, Wirovest used in this study was subjected to four different drying methods. A total of 80 specimens were prepared in a cylindrical form; 20 specimens were air dried for 2 h, 20 specimens were dried in a conventional oven at 230°C for 1 h, 20 specimens were dried in microwave oven at 600 W for 10 min, and remaining 20 specimens were dried first in microwave oven and then in conventional oven. The dried specimens were tested at 2-h interval for diametral compression at a crosshead speed of 0.5 cm/min.
Pairwise analysis.
The microwave drying technique and drying by combination method resulted in greater DTS, respectively.
Within the limitation of this study, PBI specimens dried in microwave oven at 600W for 10 min increased the diametral strength and are also a time-saving procedure.
本研究评估并比较了用于可摘局部义齿制作的无环磷酸盐粘结包埋材料(PBI)的径向拉伸强度(DTS)。
对比研究。
本研究中使用的PBI材料Wirovest采用四种不同的干燥方法。总共制备了80个圆柱形试件;20个试件空气干燥2小时,20个试件在传统烤箱中于230°C干燥1小时,20个试件在微波炉中以600W干燥10分钟,其余20个试件先在微波炉中干燥,然后在传统烤箱中干燥。干燥后的试件每隔2小时以0.5厘米/分钟的十字头速度进行径向压缩测试。
成对分析。
微波干燥技术和组合干燥法分别产生了更高的径向拉伸强度。
在本研究的限制范围内,在微波炉中以600W干燥10分钟的PBI试件提高了径向强度,并且也是一种节省时间的方法。