Kim Young Kyung, Hong Mi-Hee, Kwon Tae-Yub
Department of Conservative Dentistry, School of Dentistry, Kyungpook National University, Daegu 41940, Korea.
Department of Orthodontics, School of Dentistry, Kyungpook National University, Daegu 41940, Korea.
Materials (Basel). 2020 Jan 8;13(2):293. doi: 10.3390/ma13020293.
The purpose of this study was to evaluate whether the incorporation of an acidic monomer into the pulp-capping material TheraCal LC, which has a weak dentin bonding, increases the shear bond strength (SBS) to dentin. Di-2-hydroxyethyl methacryl hydrogenphosphate was incorporated into the material at 0.0 (TL0, control), 5.0 (TL5), and 10.0 (TL10) wt%. The water contact angle (CA) and mechanical properties for each material were also studied ( = 6). Debonding was performed at two different times (immediate and after 24 h) ( = 12). Hydroxyl and calcium ion releases in water at 37 °C were monitored up to 28 days ( = 6). The addition of the acidic monomer decreased the CAs ( < 0.001) and increased the flexural moduli ( < 0.001). The debonding time did not significantly affect the SBS values ( = 0.600). The TL10 group exhibited the highest SBS values, followed by the TL5 group. The TL10 group released significantly more calcium ions than the other two groups from 3 days ( < 0.05). The incorporation of the acidic monomer at 10.0 wt% into TheraCal LC enhanced bonding to dentin, while not negatively affecting the mechanical properties and ion-leaching capacity of the material.
本研究的目的是评估将酸性单体加入到牙本质粘结较弱的盖髓材料TheraCal LC中是否会提高其与牙本质的剪切粘结强度(SBS)。将甲基丙烯酸二(2 - 羟乙基)氢磷酸酯以0.0(TL0,对照组)、5.0(TL5)和10.0(TL10)wt%的比例加入到该材料中。还研究了每种材料的水接触角(CA)和力学性能(n = 6)。在两个不同时间点(即刻和24小时后)进行脱粘试验(n = 12)。监测了37℃水中羟基和钙离子的释放情况,持续28天(n = 6)。酸性单体的加入降低了水接触角(P < 0.001)并提高了弯曲模量(P < 0.001)。脱粘时间对SBS值没有显著影响(P = 0.600)。TL10组的SBS值最高,其次是TL5组。从第3天起,TL10组释放的钙离子明显多于其他两组(P < 0.05)。将10.0 wt%的酸性单体加入到TheraCal LC中可增强与牙本质的粘结,同时不会对材料的力学性能和离子溶出能力产生负面影响。