Suppr超能文献

三种不同修整和抛光技术后复合材料表面粗糙度、硬度及光泽度的评估:一项体外研究

Evaluation of Surface Roughness, Hardness, and Gloss of Composites After Three Different Finishing and Polishing Techniques: An In Vitro Study.

作者信息

Nithya Kumar, Sridevi Krishnamoorthy, Keerthi Venkatesan, Ravishankar Periasamy

机构信息

Conservative Dentistry and Endodontics, Thai Moogambigai Dental College and Hospital, Dr. M.G.R. Educational and Research Institute University, Chennai, IND.

出版信息

Cureus. 2020 Feb 19;12(2):e7037. doi: 10.7759/cureus.7037.

Abstract

Introduction The purpose of this in vitro study was to evaluate the effect of three different polishing systems on the microhardness, surface roughness, and gloss of resin composites. Materials and Methods The materials evaluated were 3M™ ESPE™ Filtek™ Z-350 XT (3M™, St. Paul, MN, USA), Grandio (Voco, Cuxhaven, Germany), 3M™ ESPE™ Filtek™ Z250 (3M™, St. Paul, MN, USA), Shofu-Beautifil Flow (Shofu, Kyoto, Japan), and RestoFill HV N-FLO (Anabond Stedman, Chennai, India). A total of 450 samples were fabricated. Three finishing and polishing systems: PoGo® (Dentsply Caulk, Milford, DE, USA), Sof-Lex Spiral, and Sof-Lex Pop-On (3M™, St Paul, MN, USA) were evaluated. Hardness, roughness, and gloss were evaluated after finishing and polishing. The surface roughness was measured with a surface profilometer, microhardness was measured with the Struers Duramin-5 microhardness tester (Struers A/S, Ballerup, Denmark) and gloss was measured using a gloss meter. The measurement values were analysed by Kolmogorov-Smirnov, Shapiro-Wilks test, and two-way ANOVA. Results The Sof-Lex Spiral group exhibited higher mean microhardness (p < 0.001), less surface roughness (p < 0.001), and higher gloss (p < 0.001). Filtek Z-250 exhibited higher mean microhardness (p < 0.001) than Grandio (p < 0.001) and Shofu Beautifil Flow (p < 0.001), and Filtek Z-350 XT exhibited more microhardness than Shofu Beautifil Flow (p < 0.001). Filtek Z-350 XT exhibited lower mean surface roughness than Filtek Z-250 (p < 0.05). Filtek Z-250 polished with Sof-Lex Spiral proved to have higher gloss (34.89 gloss units (GU)) than Grandio and RestoFill HV N-FLO (p < 0.05). Conclusions Hardest, smoothest, and glossiest surfaces were obtained with the Sof-Lex Spiral finishing/polishing system. The mean microhardness of Filtek Z-250 and Filtek Z-350 XT was found to be higher than other composites used in this study. Filtek Z-350 showed a lower mean surface roughness and Filtek Z-250 exhibited a higher mean gloss.

摘要

引言 本体外研究的目的是评估三种不同的抛光系统对树脂复合材料的显微硬度、表面粗糙度和光泽度的影响。

材料与方法 所评估的材料有3M™ ESPE™ Filtek™ Z-350 XT(美国明尼苏达州圣保罗市3M公司)、Grandio(德国库克斯港Voco公司)、3M™ ESPE™ Filtek™ Z250(美国明尼苏达州圣保罗市3M公司)、松风Beautifil Flow(日本京都松风公司)以及RestoFill HV N-FLO(印度金奈Anabond Stedman公司)。共制作了450个样本。评估了三种修整和抛光系统:PoGo®(美国特拉华州米尔福德登士柏卡ulk公司)、Sof-Lex Spiral和Sof-Lex Pop-On(美国明尼苏达州圣保罗市3M公司)。在修整和抛光后评估硬度、粗糙度和光泽度。使用表面轮廓仪测量表面粗糙度,使用Struers Duramin-5显微硬度测试仪(丹麦巴勒鲁普Struers A/S公司)测量显微硬度,并使用光泽仪测量光泽度。测量值通过柯尔莫哥洛夫-斯米尔诺夫检验、夏皮罗-威尔克检验和双向方差分析进行分析。

结果 Sof-Lex Spiral组表现出更高的平均显微硬度(p < 0.001)、更低的表面粗糙度(p < 0.001)和更高的光泽度(p < 0.001)。Filtek Z-250的平均显微硬度高于Grandio(p < 0.001)和松风Beautifil Flow(p < 0.001),Filtek Z-350 XT的显微硬度高于松风Beautifil Flow(p < 0.001)。Filtek Z-350 XT的平均表面粗糙度低于Filtek Z-250(p < 0.05)。用Sof-Lex Spiral抛光的Filtek Z-250的光泽度(34.89光泽单位(GU))高于Grandio和RestoFill HV N-FLO(p < 0.05)。

结论 使用Sof-Lex Spiral修整/抛光系统可获得最硬、最光滑和最有光泽的表面。发现Filtek Z-250和Filtek Z-350 XT的平均显微硬度高于本研究中使用的其他复合材料。Filtek Z-350的平均表面粗糙度较低,Filtek Z-250的平均光泽度较高。

相似文献

引用本文的文献

本文引用的文献

10
Resin composite--state of the art.树脂复合材料——最新技术。
Dent Mater. 2011 Jan;27(1):29-38. doi: 10.1016/j.dental.2010.10.020. Epub 2010 Nov 18.

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验