生物刺激聚左旋乳酸可注射植入物复溶后立即使用。

Immediate Use After Reconstitution of a Biostimulatory Poly-L-Lactic Acid Injectable Implant.

作者信息

Baumann Kerstin, Alm Johanna, Norberg Maria, Ejehorn Maria

出版信息

J Drugs Dermatol. 2020 Dec 1;19(12):1199-1203. doi: 10.36849/JDD.2020.5228.

Abstract

BACKGROUND

Poly-L-lactic acid (PLLA) is a biodegradable, synthetic polymer that stimulates collagen production and can improve skin quality, volume, and thickness. The current reconstitution procedure for Sculptra, a PLLA-containing injectable device involves 2 hours standing time before use.

OBJECTIVE

To evaluate and validate an immediate-use procedure for reconstituting a PLLA-containing injectable device.

METHODS AND MATERIALS

Three batches of the product were shaken for 1 minute immediately after reconstitution with 8 mL of sterile water. Different physicochemical tests including viscosity, concentration of excipients (sodium carboxymethylcellulose and mannitol), pH, and particle size distribution were performed for standing times 0, 2, 24, and 72 hours after immediate shaking, and compared with the standard 2 hours standing time before shaking. The recovery and stability of optional addition of 1 mL of 2% lidocaine hydrochloride was also assessed.

RESULTS

All physiochemical parameters evaluated were equivalent, regardless of reconstitution procedure, showing that shaking vigorously for 1 minute dissolves the excipients of the product properly without a required standing time and with no impact to the PLLA particles. There were no differences in lidocaine hydrochloride content of suspensions after 0 and 72 hours.

CONCLUSION

The PLLA-containing product can be used immediately after reconstitution including vigorous shaking, as shown from physicochemical analyses. Optional addition of lidocaine hydrochloride is feasible. J Drugs Dermatol. 2020;19(12): doi:10.36849/JDD.2020.5228.

摘要

背景

聚左旋乳酸(PLLA)是一种可生物降解的合成聚合物,可刺激胶原蛋白生成,改善皮肤质量、体积和厚度。含PLLA的注射用产品塑然雅目前的复溶程序要求在使用前静置2小时。

目的

评估并验证含PLLA注射用产品的即时使用复溶程序。

方法和材料

三批产品用8 mL无菌水复溶后立即振荡1分钟。在立即振荡后的0、2、24和72小时进行不同的物理化学测试,包括粘度、辅料(羧甲基纤维素钠和甘露醇)浓度、pH值和粒度分布,并与振荡前标准静置2小时的情况进行比较。还评估了额外添加1 mL 2%盐酸利多卡因的回收率和稳定性。

结果

无论复溶程序如何,所有评估的物理化学参数均相当,这表明剧烈振荡1分钟可使产品辅料充分溶解,无需静置时间,且对PLLA颗粒无影响。0小时和72小时后悬浮液中盐酸利多卡因含量无差异。

结论

理化分析表明,含PLLA产品复溶后(包括剧烈振荡)可立即使用。额外添加盐酸利多卡因是可行的。《药物皮肤病学杂志》。2020年;19(12):doi:10.36849/JDD.2020.5228 。