J Adv Prosthodont. 2020 Dec;12(6):344-350. doi: 10.4047/jap.2020.12.6.344. Epub 2020 Dec 28.
Recently introduced hybrid and reinforced glass ceramic computer-aided design/computer-aided manufacturing (CAD/CAM) materials have been used for full-coverage restorations. However; the effect of adjustment and type of materials on internal and marginal adaptation are unknown. This study aimed to evaluate and compare the marginal and internal adaptations of crowns made of three different CAD/CAM materials before and after adjustment.
One acrylic resin maxillary first molar was prepared and served as the master die. Thirty-six restorations were fabricated using CAD/CAM system (CEREC Omnicam, MCXL) with three materials including lithium disilicate (IPS e.max CAD), zirconia-reinforced lithium silicate (Suprinity), and hybrid ceramic (Enamic). Internal and marginal adaptations were evaluated with the reference point matching technique before and after adjustment. The data were analyzed using mixed ANOVA considering α=.05 as the significance level.
The effect of adjustment and its interaction with the restoration material were significant for marginal, absolute marginal, and occlusal discrepancies (<.05). Before adjustment, Suprinity had lower marginal discrepancies than IPS e.max CAD (=.18) and Enamic (=.021); though no significant differences existed after adjustment.
Within the limitations of this study, crowns fabricated from IPS e.max CAD and Suprinity resulted in slightly better adaptation compared with Enamic crowns before adjustment. However, marginal, axial, and occlusal discrepancies were similar among all materials after the adjustment.
最近推出的混合增强型玻璃陶瓷计算机辅助设计/计算机辅助制造(CAD/CAM)材料已用于全冠修复。然而,材料的调改及其类型对内部和边缘适合性的影响尚不清楚。本研究旨在评估和比较三种不同CAD/CAM材料制作的全冠在调改前后的边缘和内部适合性。
制备一颗丙烯酸树脂上颌第一磨牙作为母模。使用CAD/CAM系统(CEREC Omnicam,MCXL)用三种材料制作36个修复体,这三种材料包括二硅酸锂(IPS e.max CAD)、氧化锆增强硅酸锂(Suprinity)和混合陶瓷(Enamic)。在调改前后采用参考点匹配技术评估内部和边缘适合性。以α = 0.05作为显著性水平,使用混合方差分析对数据进行分析。
调改及其与修复材料的交互作用对边缘、绝对边缘和咬合差异具有显著影响(P < 0.05)。调改前,Suprinity的边缘差异低于IPS e.max CAD(P = 0.18)和Enamic(P = 0.021);但调改后无显著差异。
在本研究的局限性内,与调改前的Enamic全冠相比,由IPS e.max CAD和Suprinity制作的全冠具有稍好的适合性。然而,调改后所有材料的边缘、轴向和咬合差异相似。