具有高负载碳纳米管/纳米纤维-多硫化物阴极的贫电解质锂硫电化学电池。

Lean-electrolyte lithium-sulfur electrochemical cells with high-loading carbon nanotube/nanofiber-polysulfide cathodes.

作者信息

Yen Yin-Ju, Chung Sheng-Heng

机构信息

Department of Materials Science and Engineering, National Cheng Kung University, No. 1, University Road, Tainan City 701, Taiwan.

出版信息

Chem Commun (Camb). 2021 Feb 25;57(16):2009-2012. doi: 10.1039/d0cc08276g. Epub 2021 Jan 28.

Abstract

A carbon nanotube/nanofiber (CNT/CNF) composite is applied as a cathode substrate to develop a high-loading polysulfide cathode (8.64 mg cm, 68 wt% sulfur). The high-loading CNT/CNF-polysulfide cathode demonstrates high energy densities (11.4-15.7 mW h cm) and long-term cyclability (200 cycles) with low electrolyte-to-sulfur (E/S) ratios of 4-7 μL mg.

摘要

一种碳纳米管/纳米纤维(CNT/CNF)复合材料被用作阴极基底,以开发一种高负载量的多硫化物阴极(8.64毫克/平方厘米,68重量%硫)。这种高负载量的CNT/CNF-多硫化物阴极在低电解液与硫(E/S)比为4 - 7微升/毫克的情况下,展现出高能量密度(11.4 - 15.7毫瓦时/平方厘米)和长期循环稳定性(200次循环)。