含银羟基磷灰石涂层与万古霉素联合应用对耐甲氧西林金黄色葡萄球菌生物膜体外形成的时间依赖性疗效。

Time-dependent efficacy of combination of silver-containing hydroxyapatite coating and vancomycin on methicillin-resistant Staphylococcus aureus biofilm formation in vitro.

作者信息

Hashimoto Akira, Miyamoto Hiroshi, Kii Sakumo, Kobatake Tomoki, Shobuike Takeo, Noda Iwao, Sonohata Motoki, Mawatari Masaaki

机构信息

Department of Orthopaedic Surgery, Faculty of Medicine, Saga University, Nabeshima 5-1-1, Saga, 849-8501, Japan.

Department of Pathology and Microbiology, Faculty of Medicine, Saga University, Nabeshima 5-1-1, Saga, 849-8501, Japan.

出版信息

BMC Res Notes. 2021 Mar 2;14(1):81. doi: 10.1186/s13104-021-05499-7.

Abstract

OBJECTIVE

We developed a silver-containing hydroxyapatite (Ag-HA) coating to prevent periprosthetic joint infection (PJI). Methicillin-resistant Staphylococcus aureus (MRSA) is the main PJI-causing bacteria. Previously, we had reported the combined effect of Ag-HA coating and vancomycin (VCM) on MRSA biofilm formation 24 h after MRSA inoculation. In this study, we investigated the time-dependent efficacy of Ag-HA coating and VCM on MRSA biofilm formation on Ti discs in vitro by three-dimensional confocal laser scanning microscopic analysis.

RESULTS

For the Ti VCM and HA VCM groups, the total biofilm volumes per area at 96 h after MRSA inoculation were significantly larger than those at 48 h after MRSA inoculation, respectively (p < 0.001). In contrast, for the Ag-HA VCM group, the total biofilm volume per area at 96 h was significantly smaller than that at 48 h (p < 0.0001). Moreover, 96 h after MRSA inoculation, the total biofilm volume per area of the Ag-HA VCM groups was significantly smaller than those of the Ti VCM and HA VCM groups (p < 0.0001). Thus, the combination of Ag-HA and VCM might be useful for the prevention of MRSA-associated PJI.

摘要

目的

我们研发了一种含银羟基磷灰石(Ag-HA)涂层以预防人工关节周围感染(PJI)。耐甲氧西林金黄色葡萄球菌(MRSA)是导致PJI的主要细菌。此前,我们曾报道过Ag-HA涂层和万古霉素(VCM)对MRSA接种24小时后生物膜形成的联合作用。在本研究中,我们通过三维共聚焦激光扫描显微镜分析,研究了Ag-HA涂层和VCM在体外对钛盘上MRSA生物膜形成的时间依赖性疗效。

结果

对于钛-VCM组和羟基磷灰石-VCM组,MRSA接种96小时后每面积的生物膜总体积分别显著大于MRSA接种48小时后的生物膜总体积(p < 0.001)。相比之下,对于Ag-HA-VCM组,96小时时每面积的生物膜总体积显著小于48小时时的生物膜总体积(p < 0.0001)。此外,MRSA接种96小时后,Ag-HA-VCM组每面积的生物膜总体积显著小于钛-VCM组和羟基磷灰石-VCM组(p < 0.0001)。因此,Ag-HA和VCM的联合使用可能有助于预防与MRSA相关的PJI。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/6399/7927400/ec2775377ce4/13104_2021_5499_Fig1_HTML.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验