用于生物材料制备的无定形磷酸钙及其相关化合物。

Apatitic calcium orthophosphates and related compounds for biomaterials preparation.

作者信息

Bonel G, Heughebaert J C, Heughebaert M, Lacout J L, Lebugle A

机构信息

Laboratoire de Physico-Chimie des Solides, Ecole Nationale Supérieure de Chimie de Toulouse, France.

出版信息

Ann N Y Acad Sci. 1988;523:115-30. doi: 10.1111/j.1749-6632.1988.tb38506.x.

Abstract

The authors show that to obtain well chemically defined apatitic bioceramics and to know the possible transformations of this material during sintering, it is necessary to prepare a good starting material. Moreover, they show that it is possible to prepare a new organic-inorganic phosphate compound. The precipitation of apatite in an aqueous medium at boiling temperature was studied using the methodology of experimental design. Independent variables were the volume of NH4OH in phosphate solution, the volume of NH4OH in calcium solution, and the time of precipitation; the response was the atomic Ca/P ratio of the obtained precipitate. A continuous variation of this ratio from 1.63 to 1.73 is observed. Implications of this result to the preparation of pure HA: Ca10(PO4)6(OH)2 is given. Moreover, when Ca/P greater than 1.67, HA reacts with Ca(OH)2 (after heating at 1000 degrees C in air for some days) to give rise to a single phase described as a modified HA (MHA), a Ca/P ratio of 1.75, an a value of 9.373 +/- 0.002 A, and a c value of 6.884 +/- 0.002 A. The reactivity (time versus temperature) of the MHA is described. If the precipitation of the calcium phosphate is realized at 37 degrees C in a water-ethanol medium in the presence of A2EP, a new apatite, chemically bonded to the organic molecule by pooling phosphate groups, is obtained.

摘要

作者表明,为了获得化学性质明确的磷灰石生物陶瓷,并了解该材料在烧结过程中可能发生的转变,制备优质的起始材料是必要的。此外,他们还表明可以制备一种新型有机 - 无机磷酸盐化合物。采用实验设计方法研究了在沸腾温度下磷灰石在水介质中的沉淀过程。自变量为磷酸盐溶液中NH₄OH的体积、钙溶液中NH₄OH的体积以及沉淀时间;响应值为所得沉淀物的原子Ca/P比。观察到该比值在1.63至1.73之间连续变化。给出了该结果对制备纯HA:Ca₁₀(PO₄)₆(OH)₂的影响。此外,当Ca/P大于1.67时,HA与Ca(OH)₂(在空气中1000℃加热数天后)反应生成一种单相,称为改性HA(MHA),其Ca/P比为1.75,a值为9.373±0.002 Å,c值为6.884±0.002 Å。描述了MHA的反应活性(时间与温度的关系)。如果在水 - 乙醇介质中,在A2EP存在下于37℃实现磷酸钙的沉淀,则可获得一种通过汇集磷酸基团与有机分子化学键合的新型磷灰石。