Chemistry Laboratory of Inorganic Materials and Applications, Faculty of Chemistry, University of Science and Technology of Oran-Mohamed Boudiaf - USTO-MB, BP.1505, 31000 El-Mnouar, Oran, Algeria E-mail:
Water Sci Technol. 2021 May;83(10):2504-2517. doi: 10.2166/wst.2021.123.
The present study deals with the preparation and structural and adsorbent characterization of the ternary layered double hydroxides (LDHs; ZFA-HT) with molar ratio Zn/Al/Fe = 2/0.5/0.5 and its product calcined (ZFA-350) at 350 °C, which is examined for the removal of phosphate P(V) and chromate Cr(VI) from aqueous media. The as-obtained materials are characterized by X-ray diffraction (XRD), Fourier-transform infrared (FT-IR), thermogravimetric analysis-differential scanning calorimetry (TGA-DSC), scanning electron microscopy-X-ray energy dispersion (SEM-EDX) and Brunauer-Emmett-Teller (BET). Structural characterizations show that the LDHs is successfully synthesized and its calcined product is a mixed oxide. Batch sorption studies are conducted to investigate the effects of various experimental parameters such as contact time, solution pH, adsorbent amount, initial P(V) or Cr(VI) concentration and temperature. The isotherms, kinetics and thermodynamic parameters of adsorption of phosphate and chromium are studied. The adsorption processes are well described by the pseudo-second-order kinetic model than the other models examined. The adsorption isotherms data fit best to the Langmuir isotherm model instead of Freundlich and Dubinin-Radushkevich models. The maximum monolayer adsorption capacity of ZFA-350 was found to be 140.85 mg/g for P(V) and 52.63 mg/g for Cr(VI). The positive ΔH and ΔS and negative ΔG values reveal that the P(V) and Cr(VI) sorption onto ZFA-350 is endothermic, irreversible and spontaneous in nature.
本研究涉及三元层状双氢氧化物(LDHs;ZFA-HT)的制备及其结构和吸附剂特性,其摩尔比为 Zn/Al/Fe = 2/0.5/0.5,其煅烧产物(ZFA-350)在 350°C 下煅烧,用于从水溶液中去除磷酸盐 P(V) 和铬酸盐 Cr(VI)。所得到的材料通过 X 射线衍射(XRD)、傅里叶变换红外(FT-IR)、热重分析-差示扫描量热法(TGA-DSC)、扫描电子显微镜-能量色散 X 射线(SEM-EDX)和 Brunauer-Emmett-Teller(BET)进行表征。结构表征表明 LDHs 成功合成,其煅烧产物为混合氧化物。进行了批量吸附研究,以研究各种实验参数的影响,如接触时间、溶液 pH 值、吸附剂用量、初始 P(V)或 Cr(VI)浓度和温度。研究了吸附磷和铬的等温线、动力学和热力学参数。吸附过程由准二级动力学模型比其他检查的模型更好地描述。吸附等温线数据最符合 Langmuir 等温线模型,而不是 Freundlich 和 Dubinin-Radushkevich 模型。ZFA-350 的最大单层吸附容量发现为 140.85 mg/g 用于 P(V)和 52.63 mg/g 用于 Cr(VI)。正的 ΔH 和 ΔS 值和负的 ΔG 值表明 P(V)和 Cr(VI)在 ZFA-350 上的吸附是吸热、不可逆和自发的。