Collins W E, Mosher D F, Diwan A R, Murthy K D, Simmons S R, Albrecht R M, Cooper S L
Department of Chemical Engineering, University of Wisconsin, Madison 53706.
Scanning Microsc. 1987 Dec;1(4):1669-76.
Temporal platelet deposition profiles of canine plasma fibronectin (CPFN) adsorbed to different polymers ex vivo and the in vitro characteristics of CPFN adsorption were studied in an attempt to correlate the two. The maximum platelet deposition (gamma pltmax) obtained at a protein preadsorption time of 30 min was greater than that obtained using an adsorption time of 120 min for all surfaces studied. At 30 min of preadsorption, gamma pltmax was 520,560 and 1230 platelets/1000 micron2 on Biomer, polyethylene (PE) and oxidized PE (OXPE), respectively. In contrast, the platelet deposition at 120 min. of fibronectin preadsorption was about 60 approximately 90 platelets/1000 micron2 on all polymers studied. The surface concentrations of adsorbed CPFN measured using 125I-CPFN, were in the order PE greater than OXPE greater than Biomer. The adsorbed protein concentration increased with increasing adsorption time. The surface distribution of adsorbed CPFN was visualized with antibody-labelled colloidal gold and scanning electron microscopy. The extent of staining was lowest on PE, greater on Biomer, and highest on OXPE, roughly similar to the order of platelet deposition. Platelet deposition ex vivo appears to correlate with the immunogold-stainable-adsorbed protein rather than with the total amount of adsorbed protein.