含整体结晶防水外加剂的结构砂浆的早期密封能力

Early Age Sealing Capacity of Structural Mortar with Integral Crystalline Waterproofing Admixture.

作者信息

Mircea Calin, Toader Tudor-Panfil, Hegyi Andreea, Ionescu Brăduț-Alexandru, Mircea Andreea

机构信息

Civil Engineering Faculty, Technical University of Cluj-Napoca, 28 Memorandumului Street, 400114 Cluj-Napoca, Romania.

NIRD URBAN-INCERC Cluj-Napoca Branch, 117 Calea Floressti, 400524 Cluj-Napoca, Romania.

出版信息

Materials (Basel). 2021 Aug 30;14(17):4951. doi: 10.3390/ma14174951.

Abstract

Crystalline admixtures embedded in concrete may react in the presence of water and generate thin crystals able to fill pores, capillaries and micro-cracks. Once the concrete has dried, the crystalline chemicals sit dormant until another dose of water starts the crystallization again. The research aims to analyses the early age self-sealing effect of a crystalline admixture at a dosage rate of 1-3% of the cement mass. Specimens made with two types of gravel were pre-loaded with three-point bending to up to 90% of the ultimate capacity, and conditioned through wet-dry cycles. Micro-crack closure was measured with a microscope after pre-loading, and after 1 day, 4 days, 8 days, 14 days and 20 days of wet-dry exposure. The results show that an admixture content of 3% achieves the best early self-sealing performance. These results are also confirmed by probabilistic analyses, which also emphasize the self-sealing potential of lower ICW contents.

摘要

嵌入混凝土中的结晶型外加剂在有水存在的情况下可能会发生反应,并生成能够填充孔隙、毛细管和微裂缝的细晶体。混凝土干燥后,结晶化学物质处于休眠状态,直到再次接触到水才会重新开始结晶。该研究旨在分析掺量为水泥质量1%-3%的结晶型外加剂的早期自密封效果。用两种类型的碎石制成的试件进行三点弯曲预加载,直至极限承载力的90%,并通过干湿循环进行养护。在预加载后以及干湿暴露1天、4天、8天、14天和20天后,用显微镜测量微裂缝的闭合情况。结果表明,3%的外加剂掺量具有最佳的早期自密封性能。概率分析也证实了这些结果,该分析还强调了较低掺量外加剂的自密封潜力。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/30e3/8434591/1e456f2847a8/materials-14-04951-g001.jpg

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验