Chen Xuemei, Gao Jianming, Wu Ye, Wu Qihong, Luo Li
School of Architecture and Civil Engineering, Chengdu University, Chengdu 610106, China.
Jiangsu Key Laboratory of Construction Materials, School of Materials Science and Engineering, Southeast University, Nanjing 211189, China.
Materials (Basel). 2022 Apr 6;15(7):2691. doi: 10.3390/ma15072691.
Calcium sulfate hemihydrate whiskers (CSHW), a multi-functional and high value-added building material, were prepared with flue gas desulfurization (FGD) gypsum by hydrothermal method, which could be a reasonable disposal of FGD gypsum. In order to obtain CSHW of a high aspect ratio, a series of manufacturing parameters such as reaction temperature, stirring speed, material-water ratio, and reaction time were investigated. The effect of stabilizing treatment and glycerol concentration on CSHW morphology were also studied by environmental scanning electron microscopy (ESEM) and statistical analysis. The results showed that the optimum preparing conditions of reaction temperature, stirring speed, water-material ratio, and reaction time were 160 °C, 200~300 rpm, 11:1 and 1 h, respectively. Furthermore, stabilizing treatment with octodecyl betaine was necessary for the preparation of CSHW. The final prepared whiskers had smooth surface, uniform morphology, a diameter of 260 nm, and a corresponding aspect ratio of 208.2. Moreover, the addition of glycerol reduced the activity of water, contributing to a lower reaction temperature and much smaller diameter.
半水硫酸钙晶须(CSHW)是一种多功能、高附加值的建筑材料,采用水热法以烟气脱硫(FGD)石膏为原料制备而成,这是一种合理处置FGD石膏的方法。为了获得高长径比的CSHW,研究了一系列制造参数,如反应温度、搅拌速度、物料水比和反应时间。还通过环境扫描电子显微镜(ESEM)和统计分析研究了稳定化处理和甘油浓度对CSHW形态的影响。结果表明,反应温度、搅拌速度、水料比和反应时间的最佳制备条件分别为160℃、200~300 rpm、11:1和1 h。此外,用十八烷基甜菜碱进行稳定化处理对于CSHW的制备是必要的。最终制备的晶须表面光滑,形态均匀,直径为260 nm,相应的长径比为208.2。此外,甘油的加入降低了水的活性,有助于降低反应温度并使直径更小。