使用磷酸盐和镁源同时固定电解锰渣中的铵根和锰。

Simultaneous immobilization of NH and Mn from electrolytic manganese residue using phosphate and magnesium sources.

作者信息

Chen Hongliang, Long Qian, Zhang Yutao, Qin Lan

机构信息

College of Chemistry and Chemical Engineering, Anshun University No. 25 Xueyuan Road, Anshun Xixiu Zone Anshun Guizhou 561000 PR China

Engineering Technology Centre of Control and Remediation of Soil Contamination of Guizhou Provincial Science & Technology Bureau, Anshun University Anshun Guizhou 561000 PR China.

出版信息

RSC Adv. 2019 Feb 6;9(8):4583-4590. doi: 10.1039/c8ra09615e. eCollection 2019 Jan 30.

Abstract

Immobilization of contaminants from electrolytic manganese residue (EMR) is essential for the safe stacking and reuse of EMR. This study provides experiment results for the simultaneous immobilization of NH and Mn from EMR using NaPO·12HO and MgSO·7HO (PS) agents, as well as NaPO·12HO and MgO (PO) agents. The optimum reaction conditions, characteristics of immobilization, mechanism and the economy of alternative chemicals were determined and are discussed. The results indicated that the immobilization efficiencies of NH and Mn were 92.4% and 99.9% respectively under the following conditions: a MgSO·7HO : NaPO·12HO : EMR mass ratio of 0.113 : 0.175 : 1, a CaO : EMR mass ratio of 0.03 : 1 and a reaction time of 1 h using PS agents. The concentration of NH in the leach liquor reduced from 1264 to 98 mg L after immobilization. The concentration of heavy metal ions decreased sharply in the leach liquor and met the Integrated Wastewater Discharge Standard of China (GB8978-1996). The characteristics of immobilization indicated that NH was immobilized to form NHMgPO·6HO and that Mn was immobilized to form Mn(PO)(OH), Mn(PO)·3HO and Mn(OH). An economic evaluation showed that using PS agents had lower associated cost than using PO agents.

摘要

固定电解锰渣(EMR)中的污染物对于EMR的安全堆放和再利用至关重要。本研究给出了使用Na₃PO₄·12H₂O和MgSO₄·7H₂O(PS)试剂以及Na₃PO₄·12H₂O和MgO(PO)试剂同时固定EMR中NH₄⁺和Mn的实验结果。确定并讨论了最佳反应条件、固定特性、机理以及替代化学品的经济性。结果表明,在以下条件下,NH₄⁺和Mn的固定效率分别为92.4%和99.9%:使用PS试剂时,MgSO₄·7H₂O∶Na₃PO₄·12H₂O∶EMR质量比为0.113∶0.175∶1,CaO∶EMR质量比为0.03∶1,反应时间为1小时。固定后浸出液中NH₄⁺的浓度从1264降至98 mg/L。浸出液中重金属离子浓度急剧下降,达到中国《污水综合排放标准》(GB8978 - 1996)。固定特性表明,NH₄⁺被固定形成NH₄MgPO₄·6H₂O,Mn被固定形成Mn₃(PO₄)₂(OH)₂、Mn₃(PO₄)₂·3H₂O和Mn(OH)₂。经济评估表明,使用PS试剂的相关成本低于使用PO试剂。