Li Haoran, Liu Chenglian, Wang Yan, Zheng Jiajun, Fan Binbin, Li Ruifeng
College of Chemistry and Chemical Engineering, Taiyuan University of Technology Taiyuan 030024 China
RSC Adv. 2018 Aug 14;8(51):28909-28917. doi: 10.1039/c8ra04858d.
ZSM-48 and ZSM-22 zeolites with similar Si/Al molar ratio have been treated with alkali to modify the pore structures and acidity, and alkali treated ZSM-22 and ZSM-48 samples have been characterized by X-ray Diffraction (XRD), Scanning Electron Microscopy (SEM), Transmission Electron Microscopy (TEM), N adsorption/desorption, Nuclear Magnetic Resonance (NMR), NH-Temperature Programmed Desorption (NH-TPD) and Pyridine-Fourier Transform Infrared Spectroscopy (Py-FTIR). Characterization results indicate that NaOH treatment could improve the mesoporous structure for both ZSM-22 and ZSM-48. NaOH treatment modifies the acidity of ZSM-22 and ZSM-48 diversely. The -hexane hydroisomerization performances of Pt supported protonic form ZSM-22 and ZSM-48 (Pt/HZSM-22 and Pt/HZSM-48) bifunctional catalysts have been evaluated in a fixed bed reactor. Catalytic results indicate that catalytic activity and selectivity depend on both pore structure and acidity of zeolites. In comparison of Pt/HZSM-22 and Pt/HZSM-48, Pt/HZSM-22 shows better -hexane hydroisomerization performance at relatively low temperature (<300 °C), meanwhile, at relatively high temperature (>300 °C) Pt/HZSM-48 exhibits better catalytic performance. Moreover, alkali treated Pt/HZSM-48 could produce more di-branched isomer compared with alkali treated Pt/HZSM-22.
具有相似硅铝摩尔比的ZSM - 48和ZSM - 22沸石已用碱处理以改变其孔结构和酸性,并且已通过X射线衍射(XRD)、扫描电子显微镜(SEM)、透射电子显微镜(TEM)、N吸附/脱附、核磁共振(NMR)、氨程序升温脱附(NH - TPD)和吡啶 - 傅里叶变换红外光谱(Py - FTIR)对碱处理的ZSM - 22和ZSM - 48样品进行了表征。表征结果表明,NaOH处理可以改善ZSM - 22和ZSM - 48两者的介孔结构。NaOH处理对ZSM - 22和ZSM - 48的酸性有不同的影响。在固定床反应器中评估了负载铂的质子型ZSM - 22和ZSM - 48(Pt/HZSM - 22和Pt/HZSM - 48)双功能催化剂的正己烷加氢异构化性能。催化结果表明,催化活性和选择性取决于沸石的孔结构和酸性。在Pt/HZSM - 22和Pt/HZSM - 48的比较中,Pt/HZSM - 22在相对低温(<300°C)下表现出更好的正己烷加氢异构化性能,同时,在相对高温(>300°C)下Pt/HZSM - 48表现出更好的催化性能。此外,与碱处理的Pt/HZSM - 22相比,碱处理的Pt/HZSM - 48可以产生更多的二支链异构体。