Millán Ramírez Ginneth Patricia, Byliński Hubert, Niedostatkiewicz Maciej
Department of Engineering Structures, Faculty of Civil and Environmental Engineering, Gdansk University of Technology, 11/12 Narutowicza street, 80-226, Gdańsk, Poland.
Sci Rep. 2022 Aug 11;12(1):13647. doi: 10.1038/s41598-022-18022-0.
This paper assesses the behavior of mineral, epoxy (EP), solvent, and water-soluble coatings when exposed to salt and regular water for 28 days. Also, it evaluates the pull-off adhesion strength of the same coating materials applied to concrete slabs saturated with oil and water and dried with two different processes: air-dried for 28 days and air-dried for 14 days plus 14 days in the oven at 70 °C. Properties such as carbonation, water absorption rate, pull-off adhesion strength were evaluated for all coatings, and tensile strength, Young's modulus, and elongation percentage were calculated for mineral coatings. According to the results, the EP coating showed the best performance with the highest pull-off adhesion strength (2.55 MPa) and lowest absorption rate, about 0.02 ± 0.002 g/m day in saltwater and 0.03 ± 0.002 g/m day in regular water. In addition, EP coatings also presented the lowest carbonation rate and the highest suppress ratio. The excellent performance of epoxy coatings is mainly due to their low porosity and the ability to decrease chloride diffusion, making them better than other types of coatings investigated in this study.
本文评估了矿物涂层、环氧(EP)涂层、溶剂型涂层和水溶性涂层在盐溶液和普通水中暴露28天的性能。此外,还评估了相同涂层材料应用于用两种不同工艺干燥的、被油和水饱和的混凝土板上的拉拔粘结强度:在空气中干燥28天以及在空气中干燥14天然后在70°C烘箱中干燥14天。对所有涂层评估了碳化、吸水率、拉拔粘结强度等性能,并计算了矿物涂层的拉伸强度、杨氏模量和伸长率。根据结果,EP涂层表现出最佳性能,具有最高的拉拔粘结强度(2.55MPa)和最低的吸水率,在盐水中约为0.02±0.002g/m·天,在普通水中约为0.03±0.002g/m·天。此外,EP涂层还呈现出最低的碳化率和最高的抑制率。环氧涂层的优异性能主要归因于其低孔隙率以及降低氯离子扩散的能力,使其优于本研究中所研究的其他类型涂层。