BIM Engineering Center of Anhui Province, Anhui Jianzhu University, Hefei 230601, China.
Anhui Jianzhu University, Hefei 230601, China.
J Environ Public Health. 2022 Aug 22;2022:9379135. doi: 10.1155/2022/9379135. eCollection 2022.
A prefabricated concrete structure is a building structure designed for sustainability and low comprehensive carbon emission. The grouted sleeve splice is a major connection method for prefabricated concrete structures. However, construction defects occur easily in the grouted sleeve splice connection at construction sites because of complex construction environments and the high connection accuracy. To determine the influence of rebar in steel half-grouted sleeve connections with construction defects, investigations were conducted using four different test groups (rebar offset, rebar bended, insufficient fluidity of grout, and control group). The load-displacement curve and load-stress curve were analyzed on 24 different specimens through uniaxial tension experiments. The experimental results showed that rebar fracture was the failure of specimens. The load-displacement curves consisted of elastic, yield, strength, and tight stages. The curves were similar to rebar under uniaxial tension, except for the rebar bended group. The axial stress and circumferential stress on the sleeve surface consistently followed a linear response before the specimen yield, whereas the axial stress and circumferential stress showed a rebound response after the specimen yielded. Different finite element models were established based on the different defects. Compared with the experimental results, the finite element analysis results coincided with those of the experimental results, and the errors were within 8% to evaluate the performance of steel half-grouted sleeve connections in construction.
预制混凝土结构是一种为可持续性和低综合碳排放而设计的建筑结构。套筒灌浆连接是预制混凝土结构的主要连接方式。然而,由于施工环境复杂和连接精度要求高,预制混凝土结构在施工现场的套筒灌浆连接中容易出现施工缺陷。为了确定施工缺陷对带半灌浆套筒的钢筋连接的影响,进行了四项不同试验组(钢筋偏置、钢筋弯曲、灌浆不流动和对照组)的研究。通过单向拉伸试验对 24 个不同的试件进行了分析,得到了荷载-位移曲线和荷载-应变曲线。试验结果表明,钢筋断裂是试件的破坏形式。荷载-位移曲线包括弹性、屈服、强度和紧密阶段。除了钢筋弯曲组外,曲线与钢筋的单向拉伸相似。在试件屈服之前,套筒表面的轴向应力和环向应力始终呈线性响应,而在试件屈服之后,轴向应力和环向应力呈回弹响应。基于不同的缺陷建立了不同的有限元模型。与试验结果相比,有限元分析结果与试验结果吻合较好,误差在 8%以内,可用于评估施工中带半灌浆套筒的钢筋连接的性能。