Graduate Program in Dentistry, School of Dentistry, Federal University of Rio Grande do Sul, Rua Ramiro Barcelos, 2492, Santa Cecília, Porto Alegre, Brazil.
Postgraduate Program in Dentistry, Federal University of Juiz de Fora, Juiz de Fora, Brazil.
J Dent. 2022 Nov;126:104283. doi: 10.1016/j.jdent.2022.104283. Epub 2022 Sep 8.
This review evaluated the effects of the acidic composition of self-etch (SE) adhesives at the long-term bond strengths to dentin and enamel.
The review followed the PRISMA Extension Statement for network meta-analysis. Studies were identified by a systematic search in PubMed, Web of Science, and Scopus databases.
The inclusion criteria were in vitro studies that evaluated bond strength data of samples analyzed at both immediate and long-term (after aging simulation) periods and that were bonded to sound dentin/enamel using SE adhesives, with at least one group of adhesives being based on 10-MDP (10-methacryloyloxy-decyl-dihydrogen-phosphate; control) and the other group being comprised of alternative acidic monomers. Statistical analyses were conducted using two methods: standard pairwise meta-analysis (SPMA) and Bayesian network meta-analysis (NMA). Heterogeneity was assessed by using the Cochran Q test and I statistics.
From 5220 studies identified, 87 met the eligibility criteria and 83 were meta-analyzed. Seventeen adhesives were based on 10-MDP and 44 systems were based on alternative acids. The resin-dentin/enamel bonds were predominantly reduced after aging (∼84% of cases). From the SPMA findings, the following acidic compositions showed lower bond strength values (effect size: mean difference [MD] with 95% confidence interval [95% CI]) than 10-MDP: 4-META (MD -4.99, 95% CI: -7.21, -2.78; p<0.001); sulfonic acids (MD -9.59, 95% CI -12.19, -6.98; p<0.001); unspecified phosphate esters (MD -8.89, 95% CI -17.50, -0.28; p = 0.04); or mixed acids (MD -11.0, 95% CI -13.62, -8.38; p<0.001). The dental bonds were benefited from the presence of 10-MDP upon longer aging (>6 months). From the NMA probabilistic findings, adhesives based on 10-MDP and phosphonic acids ranked as having the best and the worst bonding potential to dentin, respectively. More than one composition (phosphonic acids and mixed acids) ranked similarly to 10-MDP in enamel. The studies scored as having moderate risk of bias (58.6%), followed by low (39.1%) and high (2.3%) risk of bias.
10-MDP is an outstanding acidic monomer that contributes to higher bonds to dentin at the long-term. In enamel, there is no evidence that one acidic composition prevails over the other.
The acidic composition of SE adhesives affects the resistance of dental bonds after simulated aging, with 10-MDP playing a significant role in the adhesion to dentin but not to the enamel.
This report is registered at the Open Science Framework (osf.io/urtdf).
本综述评估了自酸蚀(SE)胶粘剂的酸性成分对牙本质和牙釉质长期粘结强度的影响。
本综述遵循 PRISMA 扩展声明进行网络荟萃分析。通过在 PubMed、Web of Science 和 Scopus 数据库中进行系统搜索来确定研究。
纳入标准为使用 SE 胶粘剂在即时和长期(老化模拟后)阶段对样本进行粘结强度数据评估的体外研究,并且样本粘结至健康牙本质/牙釉质,至少有一组胶粘剂基于 10-MDP(10- 甲丙烯酰氧基癸基二氢磷酸酯;对照),另一组由替代酸性单体组成。使用两种方法进行统计分析:标准成对荟萃分析(SPMA)和贝叶斯网络荟萃分析(NMA)。使用 Cochran Q 检验和 I 统计量评估异质性。
从 5220 项研究中,有 87 项符合入选标准并进行了荟萃分析。有 17 种胶粘剂基于 10-MDP,44 种系统基于替代酸。树脂-牙本质/牙釉质粘结在老化后主要降低(~84%的情况)。从 SPMA 的研究结果来看,以下酸性成分的粘结强度值较低(效应大小:均值差 [MD]及其 95%置信区间 [95%CI]):4-META(MD -4.99,95%CI -7.21,-2.78;p<0.001);磺酸(MD -9.59,95%CI -12.19,-6.98;p<0.001);未指定的磷酸酯(MD -8.89,95%CI -17.50,-0.28;p = 0.04);或混合酸(MD -11.0,95%CI -13.62,-8.38;p<0.001)。在较长的老化时间(>6 个月)后,10-MDP 使牙本质的粘结受益。从 NMA 概率研究结果来看,基于 10-MDP 和膦酸的胶粘剂分别具有最佳和最差的牙本质粘结潜力。不止一种成分(膦酸和混合酸)在牙釉质中的粘结强度与 10-MDP 相似。评分显示,有 58.6%的研究为中度偏倚风险,39.1%的研究为低度偏倚风险,2.3%的研究为高度偏倚风险。
10-MDP 是一种出色的酸性单体,可在长期内提高牙本质的粘结强度。在牙釉质中,没有证据表明一种酸性成分优于另一种。
SE 胶粘剂的酸性成分会影响模拟老化后牙体粘结的耐久性,10-MDP 在牙本质粘结中起重要作用,但对牙釉质粘结无明显作用。
本报告在开放科学框架(osf.io/urtdf)注册。