Kumar Prince, Pacharne Ajay Pravin, Mishra Sunil Kumar
Department of Prosthodontics, Rama Dental College Hospital and Research Centre, Kanpur, Uttar Pradesh, India.
J Pharm Bioallied Sci. 2022 Jul;14(Suppl 1):S222-S224. doi: 10.4103/jpbs.jpbs_133_22. Epub 2022 Jul 13.
At different timings, assessment and comparison of the dimensional stability and surface hardness of three interocclusal recording materials (IRM).
Samples of polyvinyl siloxane, ZOE, and bite registration wax were made using stainless steel die. Each group had 10 samples. At 1, 8, 24, and 48 h, the samples were estimated using a 10× amplification stereo microscope.
Four readings were taken for each sample, the mean was considered to scale the dimensional change and surface hardness. At 1, 8, 24, and 48 h mean dimensional change was viewed as the most extreme among group 3 followed by group 2 and afterward group 1 ( < 0.05).
Polyvinyl siloxane was the steadiest, most precise, and had the most noteworthy surface hardness among the three interocclusal materials.
在不同时间点,评估和比较三种牙合间记录材料(IRM)的尺寸稳定性和表面硬度。
使用不锈钢模具制作聚甲基乙烯基硅氧烷、氧化锌丁香酚水门汀和咬合记录蜡的样本。每组有10个样本。在1、8、24和48小时,使用10倍放大立体显微镜对样本进行评估。
每个样本进行四次读数,取平均值以衡量尺寸变化和表面硬度。在1、8、24和48小时,第三组的平均尺寸变化被视为最极端,其次是第二组,然后是第一组(P<0.05)。
在三种牙合间材料中,聚甲基乙烯基硅氧烷最稳定、最精确,且表面硬度最高。