Biosensors (Basel). 2022 Sep 15;12(9):760. doi: 10.3390/bios12090760.
The determination of plant growth regulators is of great importance for the quality monitoring of crops. In this work, 4-bromophenoxyacetic acid (4-BPA), one of the phenoxyacetic acids, was detected via the electrochemical method for the first time. A CeO-decorated electrochemical exfoliated graphene (eGr) composite (CeO/eGr) was constructed as the sensor for sensitive detection of 4-BPA due to the synergistic effect of the excellent catalytic active sites of CeO and good electron transference of the eGr. The developed CeO/eGr sensor displayed a good linearity in a wide range from 0.3 to 150 μmol/L and the lowest detection limit of 0.06 μmol/L for 4-BPA detection. Electrochemical oxidation of 4-BPA follows a mix-controlled process on the CeO/eGr electrode, which involves 2e in the transference process. This developed CeO/eGr sensor has excellent repeatability with a relative standard deviation (RSD) of 2.35% in 10 continuous measurements. Moreover, the practical application of the sensor for 4-BPA detection in apple juice has recoveries in the range of 90-108%. This proposed CeO/eGr sensor has great potential for detecting plant growth regulators in the agricultural industry.
植物生长调节剂的测定对作物质量监测具有重要意义。在这项工作中,首次通过电化学方法检测到了苯氧乙酸中的 4-溴苯氧乙酸(4-BPA)。CeO 修饰的电化学剥离石墨烯(eGr)复合材料(CeO/eGr)由于 CeO 的优异催化活性位点和 eGr 的良好电子转移的协同效应,被构建为用于灵敏检测 4-BPA 的传感器。所开发的 CeO/eGr 传感器在 0.3 至 150 μmol/L 的宽范围内呈现出良好的线性,对于 4-BPA 检测的最低检测限为 0.06 μmol/L。4-BPA 在 CeO/eGr 电极上的电化学氧化遵循混合控制过程,其中涉及 2e 的转移过程。这种开发的 CeO/eGr 传感器具有出色的重复性,在 10 次连续测量中相对标准偏差(RSD)为 2.35%。此外,该传感器在苹果汁中用于 4-BPA 检测的实际应用具有 90-108%的回收率范围。该提出的 CeO/eGr 传感器在农业领域检测植物生长调节剂具有很大的潜力。