Roberts M W, Moffa J P, Jenkins W A
J Am Dent Assoc. 1978 Nov;97(5):829-32. doi: 10.14219/jada.archive.1978.0485.
One hundred fifty-seven fractured anterior teeth were restored with one of three acid-etch composite resin systems and were clinically and radiographically evaluated for 24 months. Of the three systems evaluated, the material activated by ultraviolet light provided the highest retention rate and clinical acceptance.
157颗前牙骨折患者使用三种酸蚀复合树脂系统之一进行修复,并进行了为期24个月的临床和影像学评估。在评估的三种系统中,紫外线激活的材料具有最高的保留率和临床接受度。